MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

3M Scotchkote™ XF 895 Fast Curing Floor Coating
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Liquid

Material Notes: Scotchkote Fast Curing Floor Coating XF 895 has been specifically developed as a high build floor protection system for application to concrete surfaces, to provide rapid return to service

Product Features:

  • Combines good application characteristics with excellent adhesion to concrete
  • Designed for application by brush or roller
  • Suitable for return to service in 1.5 hrs
  • Also suitable for use on asphalt floor surfaces in combination with 3M Scotchkote Primer FB 856

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.20 g/cc0.0434 lb/in³
Solids Content 100 %100 %
Thickness 152 - 203 microns6.00 - 8.00 mil
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 75 - 8075 - 80ASTM D2240
Tensile Strength at Break 22.6 MPa3280 psiASTM D638
Elongation at Break 15 - 20 %15 - 20 %ASTM D412
Abrasion 7878[mg] 1000 cycles
 
Processing PropertiesMetricEnglishComments
Cure Time 45.0 - 60.0 min0.750 - 1.00 hourTouch Dry
 60.0 - 90.0 min1.00 - 1.50 hourHard Dry
 10100 min168 hourFull Cure
 
Descriptive Properties
AppearanceLight Gray, Clear

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMM35316 / 170063

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.