MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

AdvanSix Aegis® H100MP Extrusion Grade Nylon 6
Categories: Polymer; Film; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Extruded

Material Notes: Description: Aegis H100MP is a lubricated and nucleated medium viscosity, nylon 6 extrusion grade homopolymer for cast or blown film. If conforms to Food and Drugs Administration requirements of 21 CFR 177.1500 as well as EU Directive 2002/72/EC. It possesses the combination of strength, toughness and thermo-forming properties associated with nylon 6 as well as excellent heat, chemical, and abrasion resistance.

Applications:

  • Processed Meat
  • Fresh Red Meat
  • Poultry
  • Fish
  • Cheese
  • Dried Food
  • Chilled Fruit Juices

Former Honeywell product; AdvanSix is a spin-off of Honeywell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Water Vapor Permeability 992 g mil/ (m2 day)
@Temperature 38.0 °C
64.0 g mil/ (100 in2 day)
@Temperature 100 °F
ASTM F1249
Specific Gravity 1.13 g/cc1.13 g/ccASTM D1505
Water Absorption <= 0.80 %<= 0.80 %Extractable Content
 1.6 %1.6 %in 24 hours
Moisture Absorption at Equilibrium 2.7 %2.7 %at 50% RH
Water Absorption at Saturation 9.5 %9.5 %
Oxygen Transmission Rate 40.3 cc/m²/day2.60 cc/100 in²/day
Nitrogen Transmission 14.0 cc-mm/m²-24hr-atm35.6 cc-mil/100 in²-24hr-atmcc/m²/day, No thickness given
Carbon Dioxide Transmission 72.8 cc-mm/m²-24hr-atm185 cc-mil/100 in²-24hr-atmcc/m²/day, No thickness given
Viscosity Measurement 3.353.3596% SAV
 100100FAV; ASTM D789
Maximum Moisture Content 0.0800.080
Melt Flow 2.6 g/10 min
@Load 1.00 kg,
Temperature 235 °C
2.6 g/10 min
@Load 2.20 lb,
Temperature 455 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 80.0 MPa11600 psiMolded; ASTM D882
Film Tensile Strength at Yield, MD 30.0 MPa4350 psiASTM D882
Film Tensile Strength at Yield, TD 30.0 MPa4350 psiASTM D882
Film Elongation at Break, MD 340 %340 %ASTM D882
Film Elongation at Break, TD 340 %340 %ASTM D882
Elongation at Break 3.8 %3.8 %Molded; ASTM D882
Tensile Modulus 0.590 GPa85.6 ksiTD; ASTM D882
 0.700 GPa102 ksiMD; ASTM D882
 3.24 GPa470 ksiMolded; ASTM D882
Flexural Strength 110 MPa16000 psiMolded; ASTM D790
Flexural Modulus 2.65 GPa384 ksiMolded; ASTM D790
Izod Impact, Notched 0.600 J/cm1.12 ft-lb/inMolded; ASTM D256
Tear Strength, Total 2070 N465 lb (f)Graves, TD; ASTM D1004
 2140 N481 lb (f)Graves, MD; ASTM D1004
Elmendorf Tear Strength MD 89700 g89700 gASTM D1922
Elmendorf Tear Strength TD 96900 g96900 gASTM D1922
Film Tensile Strength at Break, MD 90.0 MPa13100 psiASTM D882
Film Tensile Strength at Break, TD 80.0 MPa11600 psiASTM D882
 
Thermal PropertiesMetricEnglishComments
Melting Point 220 °C428 °FASTM D3418
Maximum Service Temperature, Air 61.0 °C142 °FHeat Deflection Temperature; ASTM D648
 
Processing PropertiesMetricEnglishComments
Middle Barrel Temperature 230 - 260 °C446 - 500 °FCast Film
 246 - 254 °C475 - 489 °FTubular (Blown) Film
Adapter Temperature 260 °C500 °FTubular (Blown) Film
 260 - 266 °C500 - 511 °FCast Film
Die Temperature 254 °C490 °FTubular (Blown) Film
 260 °C500 °FCast Film
Melt Temperature 240 °C464 °FMolded
 254 - 260 °C489 - 500 °FTubular (Blown) Film
 260 - 270 °C500 - 518 °FCast Film
Mold Temperature 80.0 °C176 °FMolded
Moisture Content 0.040 %0.040 %
 
Compliance PropertiesMetricEnglishComments
FDA YesYes
 
Descriptive Properties
Puncture Index470 gm/milASTM D1306, MD
Puncture Strength960 gASTM D1306, MD

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AdvanSix Aegis® HCA73MP Nylon 6/6,6 Extrusion Grade Copolymer
AdvanSix Aegis® HCA73ZP Nylon 6/6,6 Extrusion Grade Copolymer
ALM D80-ST Nylon 11 SLS Prototyping Polymer
ALM PA 850-Nat Nylon 11 SLS Prototyping Polymer
AdvanSix Aegis® H73MP Extrusion Grade Nylon 6

PALA13 / 23105

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.