MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Mateck Glass (BK7 analogous)
Categories: Ceramic; Glass; Glass Ceramic

Material Notes: Optical crystals

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.51 g/cc0.0907 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Modulus of Elasticity 81.0 GPa11700 ksi
Poissons Ratio 0.2060.206
Shear Modulus 33.6 GPa4870 ksiCalculated
 
Thermal PropertiesMetricEnglishComments
CTE, linear 7.10 µm/m-°C
@Temperature -30.0 - 70.0 °C
3.94 µin/in-°F
@Temperature -22.0 - 158 °F
Specific Heat Capacity 0.858 J/g-°C0.205 BTU/lb-°F
Thermal Conductivity 1.114 W/m-K7.731 BTU-in/hr-ft²-°F
Melting Point 559 °C1040 °F
 
Optical PropertiesMetricEnglishComments
Refractive Index  1.50731
@Wavelength 1014 nm
1.50731
@Wavelength 1014 nm
 1.51872
@Wavelength 546.1 nm
1.51872
@Wavelength 546.1 nm
at ne
 1.52283
@Wavelength 480 nm
1.52283
@Wavelength 480 nm
at nf'
 1.53626
@Wavelength 365 nm
1.53626
@Wavelength 365 nm
IR Transmittance  75 %
@Wavelength 2300 nm
75 %
@Wavelength 2300 nm
Internal Transmittance
 90 %
@Wavelength 2000 nm
90 %
@Wavelength 2000 nm
Internal Transmittance
UV Transmittance  8.0 %
@Wavelength 300 nm
8.0 %
@Wavelength 300 nm
Internal Transmittance
 92 %
@Wavelength 350 nm
92 %
@Wavelength 350 nm
Internal Transmittance
 
Descriptive Properties
Thermal Coefficient of Refractive Index2.8E-060.546 microns for ± 20°C
Transmission Range (microns)0.35 - 2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Schott N-BK7 Glass
Schott P-BK7 516641.243, Optical Glass
724-8 Nextrema® Opaque White Glass Ceramic/SCHOTT
Borosilicate Glass
Mateck Zero Expansion Glass - ZERODUR

CMAT044 / 87728

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.