Daikin-Polyflon™ PTFE F-208 is a polytetrafluoroethylene fine powder resin for paste extrusion manufactured without the use of PFOA. F-208 has been designed for small diameter coaxial cables and tubing applications that are run at high reduction ratios. F-208 is ideal for high frequency insulating applications because of its low, uniform dielectric constant and dissipation factor over a wide frequency range. F-208 has good clarity and demonstrates excellent thermal stability and dimensional tolerance at low extrusion pressures.Information provided by Daikin. |