MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Samyang Trirex® PC-3025G10-N(R) 10% Glass Reinforced Clear Flame Retardant Polycarbonate With Release  (discontinued **)
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Glass Fiber Filled, Flame Retardant

Material Notes: Information provided by US distributor Polymer Technology and Services, LLC (PTS).

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.25 g/cc0.0452 lb/in³ASTM D792
Water Absorption 0.13 %0.13 %24 hours at 73°F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 121121ASTM D785
Tensile Strength, Yield 75.8 MPa
@Thickness 3.17 mm
11000 psi
@Thickness 0.125 in
Elongation at Break 6.0 %
@Thickness 3.17 mm
6.0 %
@Thickness 0.125 in
Flexural Yield Strength 117.2 MPa
@Thickness 3.17 mm
17000 psi
@Thickness 0.125 in
Flexural Modulus 3.38 GPa
@Thickness 3.17 mm
490 ksi
@Thickness 0.125 in
Izod Impact, Notched 1.07 J/cm
@Thickness 3.17 mm
2.00 ft-lb/in
@Thickness 0.125 in
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 143 °C289 °FASTM D648
Flammability, UL94 V-0
@Thickness 1.59 mm
V-0
@Thickness 0.0625 in
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 90 %90 %clear; thickness not quantified
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 241 - 279 °C465 - 535 °F
Middle Barrel Temperature 271 - 310 °C520 - 590 °F
Front Barrel Temperature 271 - 310 °C520 - 590 °F
Nozzle Temperature 271 - 299 °C520 - 570 °F
Melt Temperature 271 - 310 °C520 - 590 °F
Mold Temperature 71.1 - 110 °C160 - 230 °F
Drying Temperature 121 °C250 °F
Dry Time 6 hour6 hour
Injection Pressure 75.8 - 131 MPa11000 - 19000 psi
Cycle Time - Injection 1.0 - 2.5 sec1.0 - 2.5 sec
Cycle Time - Cooling 5.0 - 40 sec5.0 - 40 sec
 
Descriptive Properties
Injection Speed- Edge GateFast
Injection Speed- Tab GateFast
Injection Speed- Tunnel GateFast

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
INEOS Styrolution Zylar® 960 MBS
Kingfa JH710 G15 Flame Retardant & 15% Glass Fiber Reinforced PC
Covestro Apec® HT KU 1-9357/2 High-Heat Polycarbonate, 20% Glass Fiber
Clariant Renol PCSP0011 Polycarbonate Alloy, Glass Fiber and Glass Bead Filled
Avient Lubri-Tech™ PC-10GF/15T FRENCH GREY Polycarbonate - 10% Glass Fiber - 15% PTFE

PLBS14 / 50468

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.