MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Momentive Performance Materials 1200® Construction Sealant  (discontinued **)
Categories: Polymer; Adhesive; Thermoset; Silicone; Silicone, RTV, Construction Grade

Material Notes: One-part, premium glazing sealant for structural as well as general purpose glazing. Cure Method: Acetoxy. Tack-free time <1 hr. Peel Strength 40 lb/in. Sag/slump 0.1 in.

Data provided by the manufacturer, GE Silicones.

GE Silicones became a part of Momentive Performance Materials in 2006.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 3030ASTM D2240
Tensile Strength, Ultimate 3.30 MPa479 psiASTM D412
Tensile Strength, Yield 0.240 MPa34.8 psiat 50% Extension (0.5 x 0.38 x 2 in bead)
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 204 °C399 °FElasticity is retained to this temperature.
Minimum Service Temperature, Air -62.0 °C-79.6 °FElasticity is retained to this temperature.
 
Processing PropertiesMetricEnglishComments
Processing Temperature 27.0 °C80.6 °FCure time to 0.38 in. is 5-7 days

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Epoxy Cure Resin
Overview of materials for Silicone, RTV, Construction Grade
Momentive Performance Materials Ultraglaze® 4400 Construction Sealant
Momentive Performance Materials TSE3331 Dark Gray Thermally Conductive Potting/Encapsulating Compound
Momentive Performance Materials Sanitary 1700™ Construction Sealant

PZZGE907 / 40461

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.