Lumicene® mPE M 3581 UV is a second generation metallocene medium density polyethylene with hexene as comonomer. Lumicene® mPE M 3581 UV is intended for the manufacture of rotomolded items. Its specific molecular structure ensures: - Superior mechanical properties
- Outstanding optical properties (gloss)
- Improved dimensional stability
- Easy processing
This former Total Petrochemicals grade is now a part of the Bayport Polymers joint venture. |