MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Hexcel® HexPly® F263 Epoxy Resin, 7781 Glass Fabric
Categories: Polymer; Thermoset; Epoxy; Epoxy/Glass SMC

Material Notes: Hexcel designation: 7781-38"-F263; Fiber: 75-1/0

Information provided by HexCel

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Filler Content 45.0 %45.0 %Laminate Fiber Volume
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield  385 MPa
@Temperature 177 °C
55800 psi
@Temperature 351 °F
 461 MPa
@Temperature 24.0 °C
66900 psi
@Temperature 75.2 °F
Tensile Modulus  23.9 GPa
@Temperature 177 °C
3470 ksi
@Temperature 351 °F
 29.7 GPa
@Temperature 24.0 °C
4310 ksi
@Temperature 75.2 °F
Compressive Yield Strength  353 MPa
@Temperature 177 °C
51200 psi
@Temperature 351 °F
 491 MPa
@Temperature 24.0 °C
71200 psi
@Temperature 75.2 °F
Compressive Modulus  26.4 GPa
@Temperature 177 °C
3830 ksi
@Temperature 351 °F
 29.7 GPa
@Temperature 24.0 °C
4310 ksi
@Temperature 75.2 °F
Shear Strength  18.0 MPa
@Temperature 177 °C
2610 psi
@Temperature 351 °F
Interlaminar
 23.0 MPa
@Temperature 24.0 °C
3340 psi
@Temperature 75.2 °F
Interlaminar
 
Descriptive Properties
Cured Thickness per Ply (cm)0.025Laminate
Dry Resin Content (%)36-40Prepreg
Flow (%)10-30

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
E-Glass Fiber, Generic
Fibre Glast 543 Style 7781 E-Glass Fiberglass Fabric
Hexcel® HexPly® F185 Epoxy Resin, 7781 Glass Fabric
Hexcel® HexForce™ 7781 Fiber Glass Fabric
Hexcel® HexForce™ 3733 Fiber Glass Fabric

PHEXC125 / 98595

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.