MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Total Lumicene® mPE M 4040 Metallocene Polyethylene, Cast Film
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Medium Density (MDPE); Medium Density Polyethylene (MDPE), Film Grade

Material Notes: Lumicene® mPE M 4040 is a Lumicene® metallocene based Polyethylene with hexene as comonomer.

Lumicene® mPE M 4040 can be processed at high output rates with low extrusion pressure, low neck-in, excellent drawability and gauge control in comparison with conventional LLDPE and first generation metallocene based polyethylene. The high stiffness combined with excellent optical properties brings a significant downgauging potential.

Lumicene® mPE M 4040 is a versatile resin that can be used in pure or in blend for the production of both mono-layer and multilayer film. Main applications are: specialty film, hygiene film, embossed film, compounds and consumer and automatic packaging, such as produce bags, mailing and hygiene overwrap film.

Information provided by Total Petrochemicals.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.940 g/cc0.940 g/ccISO 1183
Thickness 20.0 microns0.787 mil
Melt Flow 4.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
4.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 14.5 MPa2100 psiISO 527-3
Film Tensile Strength at Yield, TD 14.7 MPa2130 psiISO 527-3
Film Elongation at Break, MD 480 %480 %ISO 527-3
Film Elongation at Break, TD 610 %610 %ISO 527-3
Elmendorf Tear Strength, MD 1.10 g/micron27.9 g/milISO 6383-2
Elmendorf Tear Strength, TD 9.20 g/micron234 g/milISO 6383-2
Dart Drop Test 30.0 g0.0662 lbISO 7765-1
Film Tensile Strength at Break, MD 33.0 MPa4790 psiISO 527-3
Film Tensile Strength at Break, TD 26.0 MPa3770 psiISO 527-3
 
Thermal PropertiesMetricEnglishComments
Melting Point 126 °C259 °FISO 11357
Vicat Softening Point 122 °C252 °FISO 306
 
Optical PropertiesMetricEnglishComments
Haze 5.5 %5.5 %ISO 14782
Gloss 86 %86 %at 45°; ASTM D2457
 
Processing PropertiesMetricEnglishComments
Processing Temperature 20.0 - 60.0 °C68.0 - 140 °FChill Roll
Melt Temperature 240 - 280 °C464 - 536 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Total Lumicene® mPE M 4707 EP Metallocene Polyethylene, Blown Film
Total Lumicene® mPE M 5220 High Density Polyethylene, Blow Molding
Total Lumicene® mPE M6040 S01 Metallocene Polyethylene, Cast Film
Total Lumicene® MR10MX0 Metallocene Random Copolymer Polypropylene, Injection Molding and Injection Blow Molding
Total Lumicene® mPE M 2735 S01 Metallocene Polyethylene, Cast Film

PTOTAL778 / 130503

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.