MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Overview of materials for Nylon 66, 30% Glass Fiber Filled
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 30% Glass Fiber Filled

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% are included. Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.14 - 1.82 g/cc0.0412 - 0.0658 lb/in³Average value: 1.38 g/cc Grade Count:1207
 1.12 - 1.35 g/cc
@Temperature 260 - 295 °C
0.0405 - 0.0488 lb/in³
@Temperature 500 - 563 °F
Average value: 1.21 g/cc Grade Count:11
Filler Content 25.0 - 35.0 %25.0 - 35.0 %Average value: 29.8 % Grade Count:141
Water Absorption 0.200 - 8.00 %0.200 - 8.00 %Average value: 2.06 % Grade Count:550
Moisture Absorption at Equilibrium 0.170 - 5.70 %0.170 - 5.70 %Average value: 1.75 % Grade Count:319
 1.20 - 2.20 %
@Temperature 70.0 - 70.0 °C
1.20 - 2.20 %
@Temperature 158 - 158 °F
Average value: 1.83 % Grade Count:25
Water Absorption at Saturation 0.800 - 9.00 %0.800 - 9.00 %Average value: 5.35 % Grade Count:150
Additive Loading 25.0 - 33.0 %25.0 - 33.0 %Average value: 29.7 % Grade Count:14
Viscosity 2.90 - 50.0 cP2.90 - 50.0 cPAverage value: 7.63 cP Grade Count:10
 20.0 - 190000 cP
@Temperature 100 - 2000 °C
20.0 - 190000 cP
@Temperature 212 - 3630 °F
Average value: 9600 cP Grade Count:15
 20.0 - 190000 cP
@Shear Rate 10.0 - 10000 1/s
20.0 - 190000 cP
@Shear Rate 10.0 - 10000 1/s
Average value: 9600 cP Grade Count:15
Viscosity Test 150 cm³/g1.50 dl/gAverage value: 150 cm³/g Grade Count:6
Viscosity Number 124 - 215 cm³/g1.24 - 2.15 dl/gAverage value: 150 cm³/g Grade Count:31
Maximum Moisture Content 0.0200 - 0.2000.0200 - 0.200Average value: 0.148 Grade Count:93
 0.200 - 0.200
@Temperature 120 - 120 °C
0.200 - 0.200
@Temperature 248 - 248 °F
Average value: 0.200 Grade Count:1
 0.200 - 0.200
@Time 299 - 299 sec
0.200 - 0.200
@Time 0.0830 - 0.0830 hour
Average value: 0.200 Grade Count:1
Linear Mold Shrinkage 0.000350 - 0.0550 cm/cm0.000350 - 0.0550 in/inAverage value: 0.00451 cm/cm Grade Count:870
 0.00200 - 0.00600 cm/cm
@Temperature 80.0 - 80.0 °C
0.00200 - 0.00600 in/in
@Temperature 176 - 176 °F
Average value: 0.00417 cm/cm Grade Count:12
Linear Mold Shrinkage, Transverse 0.00100 - 0.0980 cm/cm0.00100 - 0.0980 in/inAverage value: 0.00924 cm/cm Grade Count:394
 0.00800 - 0.0100 cm/cm
@Temperature 80.0 - 80.0 °C
0.00800 - 0.0100 in/in
@Temperature 176 - 176 °F
Average value: 0.00833 cm/cm Grade Count:12
Melt Flow 1.00 - 198 g/10 min1.00 - 198 g/10 minAverage value: 29.7 g/10 min Grade Count:91
Spiral Flow 35.0 - 757 cm13.8 - 298 inAverage value: 130 cm Grade Count:15
Ash 23.0 - 36.0 %23.0 - 36.0 %Average value: 30.6 % Grade Count:28
 28.0 - 32.0 %
@Temperature 625 - 625 °C
28.0 - 32.0 %
@Temperature 1160 - 1160 °F
Average value: 30.0 % Grade Count:1
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell L 110110Average value: 110 Grade Count:4
Hardness, Rockwell M 58.0 - 12058.0 - 120Average value: 91.9 Grade Count:51
Hardness, Rockwell R 85.0 - 12585.0 - 125Average value: 116 Grade Count:186
 24.0 - 24.0
@Temperature 80.0 - 80.0 °C
24.0 - 24.0
@Temperature 176 - 176 °F
Average value: 24.0 Grade Count:2
Hardness, Shore D 77.0 - 90.077.0 - 90.0Average value: 84.0 Grade Count:13
Ball Indentation Hardness 90.0 - 280 MPa13100 - 40600 psiAverage value: 209 MPa Grade Count:64
Tensile Strength, Ultimate 19.0 - 248 MPa2760 - 36000 psiAverage value: 152 MPa Grade Count:940
 35.0 - 235 MPa
@Temperature -40.0 - 150 °C
5080 - 34100 psi
@Temperature -40.0 - 302 °F
Average value: 102 MPa Grade Count:21
Tensile Strength, Yield 18.8 - 290 MPa2730 - 42100 psiAverage value: 156 MPa Grade Count:286
 231 - 240 MPa
@Temperature -40.0 - -40.0 °C
33500 - 34800 psi
@Temperature -40.0 - -40.0 °F
Average value: 236 MPa Grade Count:2
Elongation at Break 1.00 - 190 %1.00 - 190 %Average value: 5.09 % Grade Count:1072
 2.00 - 6.80 %
@Temperature -40.0 - 150 °C
2.00 - 6.80 %
@Temperature -40.0 - 302 °F
Average value: 4.76 % Grade Count:15
Elongation at Yield 2.00 - 11.0 %2.00 - 11.0 %Average value: 3.81 % Grade Count:95
 3.50 - 6.00 %
@Temperature 60.0 - 150 °C
3.50 - 6.00 %
@Temperature 140 - 302 °F
Average value: 4.68 % Grade Count:6
Modulus of Elasticity 0.0848 - 19.7 GPa12.3 - 2850 ksiAverage value: 8.56 GPa Grade Count:680
 0.220 - 9.30792 GPa
@Temperature -40.0 - 150 °C
31.9 - 1350.02 ksi
@Temperature -40.0 - 302 °F
Average value: 4.58 GPa Grade Count:12
Flexural Yield Strength 26.2 - 331 MPa3800 - 48000 psiAverage value: 226 MPa Grade Count:914
 100 - 325 MPa
@Temperature -40.0 - 121 °C
14500 - 47100 psi
@Temperature -40.0 - 250 °F
Average value: 210 MPa Grade Count:13
Flexural Modulus 0.758 - 61.4 GPa110 - 8910 ksiAverage value: 7.95 GPa Grade Count:1005
 3.10 - 11.6 GPa
@Temperature -40.0 - 121 °C
450 - 1680 ksi
@Temperature -40.0 - 250 °F
Average value: 6.65 GPa Grade Count:15
Flexural Strain at Break 2.50 - 7.00 %2.50 - 7.00 %Average value: 4.69 % Grade Count:32
Compressive Yield Strength 28.0 - 240 MPa4060 - 34800 psiAverage value: 140 MPa Grade Count:18
 70.0 - 250 MPa
@Temperature -40.0 - 80.0 °C
10200 - 36300 psi
@Temperature -40.0 - 176 °F
Average value: 158 MPa Grade Count:2
Poissons Ratio 0.340 - 0.4000.340 - 0.400Average value: 0.362 Grade Count:68
Shear Modulus 0.0900 - 3.90 GPa13.1 - 566 ksiAverage value: 3.02 GPa Grade Count:5
Shear Strength 50.0 - 95.0 MPa7250 - 13800 psiAverage value: 77.6 MPa Grade Count:27
Izod Impact, Notched 0.450 - 75.0 J/cm0.843 - 141 ft-lb/inAverage value: 1.30 J/cm Grade Count:458
 0.500 - 3.84408 J/cm
@Temperature -40.0 - 149 °C
0.937 - 7.20154 ft-lb/in
@Temperature -40.0 - 300 °F
Average value: 1.29 J/cm Grade Count:7
 0.64068 - 2.24238 J/cm
@Temperature -40.0 - 72.8 °C
1.2003 - 4.20090 ft-lb/in
@Temperature -40.0 - 163 °F
Average value: 1.29 J/cm Grade Count:6
 0.64068 - 2.24238 J/cm
@Thickness 3.17 - 3.17 mm
1.2003 - 4.20090 ft-lb/in
@Thickness 0.125 - 0.125 in
Average value: 1.29 J/cm Grade Count:6
Izod Impact, Unnotched 0.0816 J/cm - NB0.153 ft-lb/in - NBAverage value: 8.03 J/cm Grade Count:75
 0.900 - 7.00 J/cm
@Temperature -30.0 - -30.0 °C
1.69 - 13.1 ft-lb/in
@Temperature -22.0 - -22.0 °F
Average value: 3.95 J/cm Grade Count:2
Izod Impact, Notched (ISO) 2.50 - 95.0 kJ/m²1.19 - 45.2 ft-lb/in²Average value: 12.8 kJ/m² Grade Count:409
 4.00 - 70.0 kJ/m²
@Temperature -40.0 - -30.0 °C
1.90 - 33.3 ft-lb/in²
@Temperature -40.0 - -22.0 °F
Average value: 10.9 kJ/m² Grade Count:112
Izod Impact, Unnotched (ISO) 6.50 - 21000 kJ/m²3.09 - 9990 ft-lb/in²Average value: 56.7 kJ/m² Grade Count:96
 6.00 - 95.0 kJ/m²
@Temperature -40.0 - -30.0 °C
2.86 - 45.2 ft-lb/in²
@Temperature -40.0 - -22.0 °F
Average value: 49.9 kJ/m² Grade Count:43
Charpy Impact Unnotched 0.600 J/cm² - NB2.86 ft-lb/in² - NBAverage value: 7.24 J/cm² Grade Count:522
 0.600 J/cm² - NB
@Temperature -40.0 - -20.0 °C
2.86 ft-lb/in² - NB
@Temperature -40.0 - -4.00 °F
Average value: 6.13 J/cm² Grade Count:269
 4.20 - 7.00 J/cm²
@Temperature 120 - 135 °C
20.0 - 33.3 ft-lb/in²
@Temperature 248 - 275 °F
Average value: 6.13 J/cm² Grade Count:5
 4.20 - 7.00 J/cm²
@Time 720000 - 720000 sec
20.0 - 33.3 ft-lb/in²
@Time 200 - 200 hour
Average value: 6.13 J/cm² Grade Count:5
Charpy Impact, Notched 0.250 - 12.0 J/cm²1.19 - 57.1 ft-lb/in²Average value: 1.24 J/cm² Grade Count:640
 0.294 - 8.50 J/cm²
@Temperature -40.0 - -20.0 °C
1.40 - 40.5 ft-lb/in²
@Temperature -40.0 - -4.00 °F
Average value: 1.01 J/cm² Grade Count:266
Puncture Energy 2.10 - 5.40 J1.55 - 3.98 ft-lbAverage value: 3.37 J Grade Count:15
 1.90 - 2.50 J
@Temperature -30.0 - -30.0 °C
1.40 - 1.84 ft-lb
@Temperature -22.0 - -22.0 °F
Average value: 2.07 J Grade Count:9
Coefficient of Friction 0.150 - 0.6100.150 - 0.610Average value: 0.281 Grade Count:21
Coefficient of Friction, Static 0.140 - 0.4100.140 - 0.410Average value: 0.214 Grade Count:14
Tensile Creep Modulus, 1 hour 5000 - 9350 MPa725000 - 1.36e+6 psiAverage value: 7550 MPa Grade Count:12
Tensile Creep Modulus, 1000 hours 2000 - 5620 MPa290000 - 815000 psiAverage value: 4570 MPa Grade Count:25
K (wear) Factor 26.2 - 604 x 10-8 mm³/N-M13.0 - 300 x 10-10 in³-min/ft-lb-hrAverage value: 81.2 x 10-8 mm³/N-M Grade Count:12
Limiting Pressure Velocity 0.330 - 0.701 MPa-m/sec9420 - 20000 psi-ft/minAverage value: 0.611 MPa-m/sec Grade Count:10
Taber Abrasion, mg/1000 Cycles 0.400 - 26.00.400 - 26.0Average value: 14.0 Grade Count:5
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1000 - 1.00e+18 ohm-cm1000 - 1.00e+18 ohm-cmAverage value: 7.87e+15 ohm-cm Grade Count:514
Surface Resistance 50.0 - 3.00e+16 ohm50.0 - 3.00e+16 ohmAverage value: 4.14e+14 ohm Grade Count:318
Static Decay 2.00 sec2.00 secAverage value: 2.00 sec Grade Count:7
Dielectric Constant 2.70 - 12.02.70 - 12.0Average value: 4.41 Grade Count:219
Dielectric Strength 1.97 - 90.0 kV/mm50.0 - 2290 kV/inAverage value: 30.8 kV/mm Grade Count:380
Dissipation Factor 0.00160 - 0.4600.00160 - 0.460Average value: 0.0657 Grade Count:180
Dielectric Loss Index 0.0140 - 0.1500.0140 - 0.150Average value: 0.0707 Grade Count:13
Arc Resistance 0.000 - 180 sec0.000 - 180 secAverage value: 107 sec Grade Count:47
Comparative Tracking Index 0.000 - 600 V0.000 - 600 VAverage value: 495 V Grade Count:338
Hot Wire Ignition, HWI 0.000 - 300 sec0.000 - 300 secAverage value: 23.1 sec Grade Count:35
High Amp Arc Ignition, HAI 0.000 - 187 arcs0.000 - 187 arcsAverage value: 114 arcs Grade Count:36
High Voltage Arc-Tracking Rate, HVTR 10.0 - 150 mm/min0.394 - 5.91 in/minAverage value: 24.6 mm/min Grade Count:31
 
Thermal PropertiesMetricEnglishComments
CTE, linear 3.24 - 90.0 µm/m-°C1.80 - 50.0 µin/in-°FAverage value: 30.5 µm/m-°C Grade Count:309
 9.00 - 21.0 µm/m-°C
@Temperature 55.0 - 160 °C
5.00 - 11.7 µin/in-°F
@Temperature 131 - 320 °F
Average value: 20.2 µm/m-°C Grade Count:14
 16.0 - 26.0 µm/m-°C
@Temperature 35.0 - 55.0 °C
8.89 - 14.4 µin/in-°F
@Temperature 95.0 - 131 °F
Average value: 20.2 µm/m-°C Grade Count:21
 16.0 - 26.0 µm/m-°C
@Thickness 2.00 - 2.00 mm
8.89 - 14.4 µin/in-°F
@Thickness 0.0787 - 0.0787 in
Average value: 20.2 µm/m-°C Grade Count:21
CTE, linear, Transverse to Flow 2.70 - 120 µm/m-°C1.50 - 66.7 µin/in-°FAverage value: 81.2 µm/m-°C Grade Count:132
 110 - 146 µm/m-°C
@Temperature 55.0 - 160 °C
61.1 - 81.1 µin/in-°F
@Temperature 131 - 320 °F
Average value: 135 µm/m-°C Grade Count:13
Specific Heat Capacity 0.340 - 2.35 J/g-°C0.0813 - 0.562 BTU/lb-°FAverage value: 1.54 J/g-°C Grade Count:30
 1.91 - 2.29 J/g-°C
@Temperature 260 - 295 °C
0.457 - 0.547 BTU/lb-°F
@Temperature 500 - 563 °F
Average value: 2.16 J/g-°C Grade Count:16
Thermal Conductivity 0.216 - 1.60 W/m-K1.50 - 11.1 BTU-in/hr-ft²-°FAverage value: 0.359 W/m-K Grade Count:55
 0.210 - 0.250 W/m-K
@Temperature 260 - 295 °C
1.46 - 1.74 BTU-in/hr-ft²-°F
@Temperature 500 - 563 °F
Average value: 0.218 W/m-K Grade Count:16
Melting Point 160 - 325 °C320 - 617 °FAverage value: 260 °C Grade Count:691
Maximum Service Temperature, Air 65.0 - 288 °C149 - 550 °FAverage value: 165 °C Grade Count:137
Hot Ball Pressure Test 205 - 220 °C401 - 428 °FAverage value: 210 °C Grade Count:3
Deflection Temperature at 0.46 MPa (66 psi) 120 - 297 °C248 - 567 °FAverage value: 253 °C Grade Count:514
Deflection Temperature at 1.8 MPa (264 psi) 76.0 - 285 °C169 - 545 °FAverage value: 243 °C Grade Count:933
Deflection Temperature at 8.0 MPa 65.6 - 220 °C150 - 428 °FAverage value: 153 °C Grade Count:27
Vicat Softening Point 195 - 258 °C383 - 496 °FAverage value: 243 °C Grade Count:181
Minimum Service Temperature, Air -30.0 - -20.0 °C-22.0 - -4.00 °FAverage value: -21.7 °C Grade Count:6
Glass Transition Temp, Tg 5.00 - 80.0 °C41.0 - 176 °FAverage value: 47.6 °C Grade Count:35
Decomposition Temperature 310 °C590 °FAverage value: 310 °C Grade Count:20
UL RTI, Electrical 65.0 - 160 °C149 - 320 °FAverage value: 124 °C Grade Count:56
UL RTI, Mechanical with Impact 65.0 - 160 °C149 - 320 °FAverage value: 108 °C Grade Count:52
UL RTI, Mechanical without Impact 65.0 - 140 °C149 - 284 °FAverage value: 122 °C Grade Count:49
Flammability, UL94 HB - 5VAHB - 5VAGrade Count:686
Flame Spread 0.000 - 80.0 mm/min0.000 - 3.15 in/minAverage value: 18.8 mm/min Grade Count:56
Oxygen Index 22.0 - 38.0 %22.0 - 38.0 %Average value: 26.7 % Grade Count:103
Glow Wire Test 600 - 975 °C1110 - 1790 °FAverage value: 768 °C Grade Count:169
Ignition Temperature 350 - 400 °C662 - 752 °FAverage value: 380 °C Grade Count:20
 
Processing PropertiesMetricEnglishComments
Processing Temperature 70.0 - 310 °C158 - 590 °FAverage value: 254 °C Grade Count:105
Nozzle Temperature 80.0 - 340 °C176 - 644 °FAverage value: 284 °C Grade Count:144
Die Temperature 255 - 315 °C491 - 599 °FAverage value: 293 °C Grade Count:3
Melt Temperature 210 - 340 °C410 - 644 °FAverage value: 285 °C Grade Count:570
Mold Temperature 26.7 - 160 °C80.0 - 320 °FAverage value: 86.7 °C Grade Count:618
Drying Temperature 65.6 - 130 °C150 - 266 °FAverage value: 82.4 °C Grade Count:527
Moisture Content 0.0200 - 0.200 %0.0200 - 0.200 %Average value: 0.162 % Grade Count:279
Dew Point -17.8 °C0.000 °FAverage value: -17.8 °C Grade Count:29
Injection Pressure 3.45 - 138 MPa500 - 20000 psiAverage value: 72.7 MPa Grade Count:120
Vent Depth 0.00127 - 0.00762 cm0.000500 - 0.00300 inAverage value: 0.00183 cm Grade Count:8

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Nylon 6, 30% Glass Fiber Filled
Overview of materials for Nylon 66, 20% Glass Fiber Filled
Overview of materials for Nylon 66/6, 30% Glass Fiber Reinforced
Overview of materials for Nylon 66, Unreinforced
Overview of materials for Nylon 66, 10% Glass Fiber Filled

O2513 / 78012

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.