MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

North American Slippery Elm (Red Elm) Wood
Categories: Wood and Natural Products; Wood; Hardwood

Material Notes: Ring-Porous Hardwood

Property values marked by an asterisk (*) have been taken from an unusually old reference source.

Key Words: Ulmus rubra; Lumber, Timber
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.480 g/cc0.0173 lb/in³Oven Dry Weight/Unseasoned Volume
 0.897 g/cc0.0324 lb/in³Unseasoned*
 
Mechanical PropertiesMetricEnglishComments
Hardness, Wood Indentation 2900 N652 lb (f)Side. Force required to imbed a 0.444 inch steel ball to one-half its diameter
 3300 N742 lb (f)End. Force required to imbed a 0.444 inch steel ball to one-half its diameter
Tensile Strength, Ultimate 4.48 MPa650 psiPerpendicular to Grain*
Modulus of Rupture 0.0552 GPa8.00 ksiStatic Bending*
Flexural Yield Strength 27.6 MPa4000 psiFiber Stress at Elastic Limit; Static Bending*
Flexural Modulus 8.48 GPa1230 ksiStatic Bending*
Compressive Strength 3.52 MPa510 psiPerpendicular to Grain*
 19.6 MPa2840 psiParallel to Grain*
 22.9 MPa3320 psiMax Crushing Strength Parallel to Grain*
Shear Strength 7.65 MPa1110 psiParallel to Grain*
Impact 3.43.4in-lb/in³; Work to Elastic Limit; Unseasoned Sample; Impact Bending*
 92009200psi; Fiber Stress at Elastic Limit; Unseasoned Sample; Impact Bending*
Work to Elastic Limit 0.00565 J/cm³0.820 in-lb/in³Static Bending*
Work to Maximum Load 0.106 J/cm³15.4 in-lb/in³Static Bending*
Cleavage 70.0 kN/m399 lb/inRadial surface of failure, Unseasoned*
 74.0 kN/m422 lb/inTangential surface of failure, Unseasoned*
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 0.127 W/m-K0.880 BTU-in/hr-ft²-°FOven Dry
 0.159 W/m-K1.10 BTU-in/hr-ft²-°F12% Moisture Content
Shrinkage 4.9 %4.9 %Radial; Unseasoned to Oven Dry*
 8.9 %8.9 %Tangential; Unseasoned to Oven Dry*
 13.8 %13.8 %Volumetric; Unseasoned to Oven Dry*

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
North American Black Willow Wood
American Red Maple Wood
North American Elm Wood
North American Engelmann Spruce Wood
North American Sweetgum Wood

PTSA160 / 71254

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.