MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Bayport Polymers Baystar™ D4720 High Density Polyethylene Film Resin, High Stalk Extrusion
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Medium Density (MDPE); Medium Density Polyethylene (MDPE), Film Grade

Material Notes: Medium Molecular Weight. Excellent processability, good tear and impact strength, good stiffness, excellent compatibility with LDPE and LLDPE, excellent drawdown, good moisture barrier properties.

Applications: Multiwall liner, gas flush poultry bags, mailing envelopes, heavy duty shipping sacks, fresh cut produce packaging, coextrusions.

MatWeb has a separate entry for the resin without using high stalk extrusion.

This former Total Petrochemicals grade is now a part of the Bayport Polymers joint venture.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.945 g/cc0.0341 lb/in³ASTM D792
Water Vapor Transmission 7.76 g/m²/day0.500 g/100 in²/dayASTM E96/66
Thickness 25.4 microns1.00 milas tested; with a 6:1 FLH/D ratio and a 4:1 BUR
Melt Flow 0.28 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.28 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
High Load Melt Index 20 g/10 min
@Load 21.6 kg,
Temperature 190 °C
20 g/10 min
@Load 47.6 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 24.1 MPa
@Thickness 0.0254 mm
3500 psi
@Thickness 0.00100 in
ASTM D882A
Film Tensile Strength at Yield, TD 25.5 MPa
@Thickness 0.0254 mm
3700 psi
@Thickness 0.00100 in
ASTM D882A
Film Elongation at Break, MD 600 %
@Thickness 0.0254 mm
600 %
@Thickness 0.00100 in
ASTM D882A
Film Elongation at Break, TD 700 %
@Thickness 0.0254 mm
700 %
@Thickness 0.00100 in
ASTM D882A
Elmendorf Tear Strength MD 28 g
@Thickness 0.0254 mm
28 g
@Thickness 0.00100 in
ASTM D1922
Elmendorf Tear Strength TD 530 g
@Thickness 0.0254 mm
530 g
@Thickness 0.00100 in
ASTM D1922
Dart Drop 3.94 g/micron
@Thickness 0.0254 mm
100 g/mil
@Thickness 0.00100 in
ASTM D1709A
Dart Drop Test 100 g0.221 lb1.0 mil; ASTM D1709A
Film Tensile Strength at Break, MD 4.83 MPa
@Thickness 0.0254 mm
700 psi
@Thickness 0.00100 in
ASTM D882A
Film Tensile Strength at Break, TD 39.3 MPa
@Thickness 0.0254 mm
5700 psi
@Thickness 0.00100 in
ASTM D882A
 
Thermal PropertiesMetricEnglishComments
Melting Point 129 °C264 °FASTM D3417
 
Processing PropertiesMetricEnglishComments
Melt Temperature 193 - 216 °C380 - 420 °FExtrusion
 
Descriptive Properties
ProcessFilm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PBAYST814m / 221025

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.