MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Outokumpu 904L High Performance Austenitic Stainless Steel
Categories: Metal; Ferrous Metal; Austenitic; Pressure Vessel Steel; Stainless Steel

Material Notes:

Applications:

  • Process equipment in chemical industry
  • Bleaching equipment in the pulp and paper industry
  • Flue-gas cleaning
  • Desalination
  • Seawater handling
  • Heat exchangers

Available in hot rolled plate (Quarto), hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, bar, and rod forms.

Key Words: EN 1.4539; ASTM 904L
Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 8.00 g/cc0.289 lb/in³RT
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell >= 180>= 180Hot rolled plate/Hot rolled strip/Cold rolled strip; EN 10003-1
Tensile Strength, Ultimate 600 MPa87000 psiOutokumpu Typical, Hot Rolled Plate (Quarto); EN 10002-1
 440 MPa
@Temperature 300 °C
63800 psi
@Temperature 572 °F
EN min.; EN 10002-5
 460 MPa
@Temperature 200 °C
66700 psi
@Temperature 392 °F
EN min.; EN 10002-5
 500 MPa
@Temperature 100 °C
72500 psi
@Temperature 212 °F
EN min.; EN 10002-5
Tensile Strength, Yield  220 MPa
@Strain 0.2 %
31900 psi
@Strain 0.2 %
EN min., RT; EN 10002-1
 260 MPa
@Strain 0.2 %
37700 psi
@Strain 0.2 %
Outokumpu Typical, Hot Rolled Plate (Quarto); EN 10002-1
 300 MPa
@Strain 1 %
43500 psi
@Strain 1 %
Outokumpu Typical, Hot Rolled Plate (Quarto); EN 10002-1
 125 MPa
@Strain 0.2 %,
Temperature 400 °C
18100 psi
@Strain 0.2 %,
Temperature 752 °F
EN min.; EN 10002-5
 145 MPa
@Strain 0.2 %,
Temperature 300 °C
21000 psi
@Strain 0.2 %,
Temperature 572 °F
EN min.; EN 10002-5
 155 MPa
@Strain 1 %,
Temperature 400 °C
22500 psi
@Strain 1 %,
Temperature 752 °F
EN min.; EN 10002-5
 175 MPa
@Strain 1 %,
Temperature 300 °C
25400 psi
@Strain 1 %,
Temperature 572 °F
EN min.; EN 10002-5
 175 MPa
@Strain 0.2 %,
Temperature 200 °C
25400 psi
@Strain 0.2 %,
Temperature 392 °F
EN min.; EN 10002-5
 205 MPa
@Strain 0.2 %,
Temperature 100 °C
29700 psi
@Strain 0.2 %,
Temperature 212 °F
EN min.; EN 10002-5
 205 MPa
@Strain 1 %,
Temperature 200 °C
29700 psi
@Strain 1 %,
Temperature 392 °F
EN min.; EN 10002-5
 235 MPa
@Strain 1 %,
Temperature 100 °C
34100 psi
@Strain 1 %,
Temperature 212 °F
EN min.; EN 10002-5
Elongation at Break 50 %50 %Outokumpu Typical, Hot Rolled Plate (Quarto); EN 10002-1
Modulus of Elasticity 195 GPa28300 ksiRT
 166 GPa
@Temperature 400 °C
24100 ksi
@Temperature 752 °F
Poissons Ratio 0.300.30RT
Shear Modulus 75.0 GPa10900 ksicalculated
Impact Test >= 60.0 J>= 44.3 ft-lbHot rolled plate/Hot rolled strip/Cold rolled strip; EN 10045-1
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.000100 ohm-cm0.000100 ohm-cmRT
 
Thermal PropertiesMetricEnglishComments
CTE, linear  15.8 µm/m-°C
@Temperature 100 °C
8.78 µin/in-°F
@Temperature 212 °F
 16.9 µm/m-°C
@Temperature 400 °C
9.39 µin/in-°F
@Temperature 752 °F
Specific Heat Capacity 0.450 J/g-°C0.108 BTU/lb-°FRT
Thermal Conductivity 12.0 W/m-K83.3 BTU-in/hr-ft²-°FRT
 18.0 W/m-K
@Temperature 400 °C
125 BTU-in/hr-ft²-°F
@Temperature 752 °F
 
Processing PropertiesMetricEnglishComments
Annealing Temperature 1080 - 1160 °C1980 - 2120 °FSolution Annealing
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.010 %0.010 %
Chromium, Cr 20 %20 %
Copper, Cu 1.5 %1.5 %
Iron, Fe 49.19 %49.19 %
Molybdenum, Mo 4.3 %4.3 %
Nickel, Ni 25 %25 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aluminum 2014-T6; 2014-T651
Outokumpu 254 SMO® High Performance Austenitic Stainless Steel
ATI Allegheny Ludlum Stainless Steel AL 904L™ Alloy (UNS N08904)
AISI Type 304L Stainless Steel
Outokumpu 2205 Duplex Stainless Steel

NOUTOK32 / 18747

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.