MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

SABIC CYCOLAC™ FXS610SK ABS (Europe)
Categories: Polymer; Thermoplastic; ABS Polymer

Material Notes: CYCOLAC FXS610SK is a multi purpose ABS injection moulding grade, providing a favourable balance of engineering properties. CYCOLAC FXS610SK is suitable for those applications that require sparkle colour effects.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.06 g/cc0.0383 lb/in³ISO 1183
Water Absorption 1.0 %1.0 %23°C/sat; ISO 62
Moisture Absorption 0.200 %0.200 %23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm0.0050 - 0.0070 in/inSABIC method
Melt Flow  24 g/10 min
@Load 10.0 kg,
Temperature 220 °C
24 g/10 min
@Load 22.0 lb,
Temperature 428 °F
cm³/10 min; ISO 1133
 25 g/10 min
@Load 10.0 kg,
Temperature 220 °C
25 g/10 min
@Load 22.0 lb,
Temperature 428 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 114114ISO 2039-2
Ball Indentation Hardness 98.0 MPa14200 psiISO 2039-1
Tensile Strength at Break 35.0 MPa5080 psi5 mm/min; ISO 527
 40.0 MPa5800 psi50 mm/min; ISO 527
Tensile Strength, Yield 45.0 MPa6530 psi5 mm/min; ISO 527
 50.0 MPa7250 psi50 mm/min; ISO 527
Elongation at Break 8.0 %8.0 %50 mm/min; ISO 527
 9.0 %9.0 %5 mm/min; ISO 527
Elongation at Yield 2.0 %2.0 %5 mm/min; ISO 527
 3.0 %3.0 %50 mm/min; ISO 527
Tensile Modulus 2.50 GPa363 ksi1mm/min; ISO 527
Flexural Yield Strength 74.0 MPa10700 psi2 mm/min; ISO 178
Flexural Modulus 2.50 GPa363 ksi2 mm/min; ISO 178
Izod Impact, Notched (ISO) 10.0 kJ/m²4.76 ft-lb/in²80*10*4; ISO 180/1A
 7.00 kJ/m²
@Temperature -30.0 °C
3.33 ft-lb/in²
@Temperature -22.0 °F
80*10*4; ISO 180/1A
Charpy Impact, Notched 1.00 J/cm²4.76 ft-lb/in²Edgew 80*10*4 sp=62mm; ISO 179/1eA
 0.600 J/cm²
@Temperature -30.0 °C
2.86 ft-lb/in²
@Temperature -22.0 °F
Edgew 80*10*4 sp=62mm; ISO 179/1eA
Taber Abrasion, mg/1000 Cycles 8989CS-17, 1 kg; SABIC method
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+15 ohm-cm>= 1.00e+15 ohm-cmIEC 60093
Surface Resistance >= 1.00e+15 ohm>= 1.00e+15 ohmROA; IEC 60093
Dielectric Constant  2.6
@Frequency 1e+6 Hz
2.6
@Frequency 1e+6 Hz
IEC 60250
 2.7
@Frequency 50.0 - 60.0 Hz
2.7
@Frequency 50.0 - 60.0 Hz
IEC 60250
Dielectric Strength  18.0 kV/mm
@Thickness 3.20 mm
457 kV/in
@Thickness 0.126 in
in oil; IEC 60243-1
 26.0 kV/mm
@Thickness 1.60 mm
660 kV/in
@Thickness 0.0630 in
in oil; IEC 60243-1
 35.0 kV/mm
@Thickness 0.800 mm
889 kV/in
@Thickness 0.0315 in
in oil; IEC 60243-1
Dissipation Factor  0.0040
@Frequency 50.0 - 60.0 Hz
0.0040
@Frequency 50.0 - 60.0 Hz
IEC 60250
 0.0090
@Frequency 1e+6 Hz
0.0090
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 600 V600 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 80.0 µm/m-°C
@Temperature 23.0 - 60.0 °C
44.4 µin/in-°F
@Temperature 73.4 - 140 °F
ISO 11359-2
CTE, linear, Transverse to Flow 80.0 µm/m-°C
@Temperature 23.0 - 60.0 °C
44.4 µin/in-°F
@Temperature 73.4 - 140 °F
ISO 11359-2
Thermal Conductivity 0.200 W/m-K1.39 BTU-in/hr-ft²-°FISO 8302
Hot Ball Pressure Test 75.0 °C167 °FIEC 60695-10-2
Deflection Temperature at 0.46 MPa (66 psi) 92.0 °C198 °FEdgew 120*10*4 sp=100mm; ISO 75/Be
Deflection Temperature at 1.8 MPa (264 psi) 80.0 °C176 °F1.8 MPa Edgew 120*10*4 sp=100mm; ISO 75/Ae
Vicat Softening Point 100 °C212 °FRate B/50; ISO 306
 102 °C216 °FRate B/120; ISO 306
Flammability, UL94 HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
UL 94 by SABIC-IP
Glow Wire Test 650 °C
@Thickness 1.00 mm
1200 °F
@Thickness 0.0394 in
IEC 60695-2-12
 
Processing PropertiesMetricEnglishComments
Processing Temperature 60.0 - 80.0 °C140 - 176 °FHopper Temperature
Nozzle Temperature 210 - 250 °C410 - 482 °FInjection Molding
Zone 1 200 - 240 °C392 - 464 °F
Zone 2 220 - 260 °C428 - 500 °F
Zone 3 220 - 260 °C428 - 500 °F
Melt Temperature 220 - 260 °C428 - 500 °F
Mold Temperature 40.0 - 80.0 °C104 - 176 °F
Drying Temperature 85.0 - 95.0 °C185 - 203 °FInjection Molding
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hourInjection Molding
Moisture Content 0.10 %0.10 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABI10038 / 243505

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.