MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Daikin NEOFLON® EP-620AS Extrusion/Molding Grade ETFE
Categories: Polymer; Thermoplastic; Fluoropolymer; ETFE/ECTFE; Fluorocarbon ETFE/ECTFE, Molded/Extruded

Material Notes: Neoflon® ETFE EP-620AS, conductive ETFE, was developed for extrusion and injection molding of parts with improved crack resistance.

Information provided by Daikin.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.82 - 1.88 g/cc1.82 - 1.88 g/ccASTM D-792
Melt Flow 1.8 - 4.0 g/10 min
@Temperature 297 °C
1.8 - 4.0 g/10 min
@Temperature 567 °F
ASTM D3159
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 25.0 - 35.0 MPa3630 - 5080 psiASTM D-3159
Elongation at Break >= 400 %>= 400 %ASTM D-3159
 
Thermal PropertiesMetricEnglishComments
Melting Point 218 - 222 °C424 - 432 °FASTM D3159

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Daikin NEOFLON® AP-201 PFA
Daikin NEOFLON® EP-506 Extrusion Grade ETFE
Daikin NEOFLON® EP-620 Extrusion/Molding Grade ETFE
Daikin NEOFLON® AP-210AS PFA Pellets
Daikin NEOFLON® EP-610 Extrusion/Molding Grade ETFE

PDAIJ9931 / 210002

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.