MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

A. Schulman BMC 665 Mineral Filled, Glass Reinforced Polyester
Categories: Polymer; Thermoset; Polyester, TS; Thermoset Polyester Glass and Mineral Filled BMC

Material Notes: BMC 665 molding compound is a mineral filled, glass reinforced polyester molding compound suitable for compression, transfer or stuffer injection molding. It is characterized by good moldability, oil and solvent resistance and creep resistance at elevated temperatures. Typical applications include replacements for die castings and sheet molding compounds, cylinder head covers, engine front timing covers, oil pans and structural components.

Information provided by Bulk Molding Compounds, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.67 g/cc0.0603 lb/in³ISO 1183
Water Absorption 0.080 %0.080 %ISO 62
 
Mechanical PropertiesMetricEnglishComments
Hardness, Barcol 4040
Tensile Strength 33.0 MPa4790 psiISO 527
Tensile Modulus 10.2 GPa1480 ksiISO 527
Flexural Strength 123 MPa17800 psiISO 178
Flexural Modulus 10.2 GPa1480 ksiISO 178
Compressive Strength 170 MPa24700 psiISO 604
Izod Impact, Notched (ISO) 36.0 kJ/m²17.1 ft-lb/in²ISO 179
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) >= 260 °C>= 500 °FISO 75
Flammability, UL94 HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
 
Processing PropertiesMetricEnglishComments
Processing Temperature >= 140 °C>= 284 °F
 
Descriptive Properties
ColorBlack
Glass Fiber Content20%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Cast Nylons Nycast® 6PA-Blue Nylon 6
Mitsubishi Chemical Advanced Materials Nylatron® MC 901 H. S. Type 6 (ASTM Product Data Sheet)
A. Schulman BMC Super-Tough Mineral Filled, Glass Reinforced Polyester
A. Schulman BMC T44 High Strength Mineral Filled Molding Compound
A. Schulman BMC T40-4020-AQ High Strength Arc Quenching Molding Compound

PBMC901 / 123365

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.