MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Dow UCON™ 50-HB-3520 PAG Lubricant
Categories: Fluid; Lubricant

Material Notes: A water soluble polyalkylene glycol (PAG).

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density  0.993 g/cc
@Temperature 100 °C
0.0359 lb/in³
@Temperature 212 °F
 1.04 g/cc
@Temperature 40.0 °C
0.0376 lb/in³
@Temperature 104 °F
 1.056 g/cc
@Temperature 20.0 °C
0.03815 lb/in³
@Temperature 68.0 °F
Viscosity Measurement 269269Index; ASTM D2270, IP 226
 680680ISO Viscosity Grade
 162000162000@ -18°C, [SUS], Saybolt
Saybolt Viscosity at 100°F 3520 SUS3520 SUS
Viscosity Measure 7500 cSt
@Temperature 0.000 °C
7500 cSt
@Temperature 32.0 °F
Saybolt Viscosity at 210°F 558 SUS558 SUS
Kinematic Viscosity at 40°C (104°F) 700 cSt700 cSt
Kinematic Viscosity at 100°C (212°F) 117 cSt117 cSt
Molecular Weight 3380 g/mol3380 g/mol
 
Thermal PropertiesMetricEnglishComments
CTE, linear 0.000800 µm/m-°C
@Temperature 55.0 °C
0.000444 µin/in-°F
@Temperature 131 °F
Pour Point -29.0 °C-20.2 °FASTM D97, IP 15
Flash Point 182 °C360 °FPMCC; ASTM D93, IP 34
 243 °C469 °FCOC; ASTM D93, IP 36
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.45981.4598
 
Descriptive Properties
Weight per Gallon8.81 lb

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Parker Chomerics Thermal Greases T670 High-Performance and General Duty Thermal Grease
Sinotek Materials MD-2 Graphite Emulsion
Parker Chomerics Thermal Greases T650 High-Performance and General Duty Thermal Grease

PDOW2017 / 183664

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.