MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BASF Petra® 140 BK-112 45% Glass Filled PET
Categories: Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET); Polyethylene Terephthalate (PET), Glass Fiber Filled, Flame Retardant

Material Notes: Petra 140 BK-112 is a 45% glass reinforced, pigmented black, polyethylene terephthalate (PET) injection molding compound offering an increased level of strength, stiffness, high temperature performance and dimensional stability. Resistance to creep under load is excellent and it maintains the inherent chemical and electrical properties associated with polyester.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.70 g/cc0.0614 lb/in³ISO 1183
Viscosity Measurement 0.520.52Inherent Viscosity
Linear Mold Shrinkage 0.0020 cm/cm0.0020 in/inASTM Data; MD
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 118118ASTM Test
Tensile Strength at Break 170 MPa24700 psi0.2 in/min; ASTM Test
Tensile Strength, Ultimate 170 MPa24700 psi5mm/min; ISO 527
Elongation at Break 2.0 %2.0 %5mm/min; ISO 527
 2.0 %2.0 %0.2 in/min; ASTM Test
Tensile Modulus 14.6 GPa2120 ksi1mm/min; ISO 527
Flexural Strength 278 MPa40300 psiASTM Test
Flexural Modulus 12.7 GPa1840 ksiASTM Test
 12.8 GPa1860 ksiISO Data
Izod Impact, Notched 0.900 J/cm
@Thickness 3.17 mm
1.69 ft-lb/in
@Thickness 0.125 in
ASTM Test
Izod Impact, Unnotched 8.70 J/cm16.3 ft-lb/inASTM Test
Izod Impact, Notched (ISO) 12.0 kJ/m²5.71 ft-lb/in²ISO Test
 11.5 kJ/m²
@Temperature -40.0 °C
5.47 ft-lb/in²
@Temperature -40.0 °F
ISO Test
Charpy Impact, Notched 1.15 J/cm²5.47 ft-lb/in²ISO 179
 1.40 J/cm²
@Temperature -30.0 °C
6.66 ft-lb/in²
@Temperature -22.0 °F
ISO 179
 
Thermal PropertiesMetricEnglishComments
CTE, linear 22.0 µm/m-°C
@Temperature -30.0 - 30.0 °C
12.2 µin/in-°F
@Temperature -22.0 - 86.0 °F
ASTM Test
Melting Point 245 °C473 °F10 K/min
 245 °C473 °FASTM Test
Deflection Temperature at 0.46 MPa (66 psi) 242 °C468 °FISO 75
Deflection Temperature at 1.8 MPa (264 psi) 220 °C428 °FISO 75
 224 °C435 °FASTM Test
 
Processing PropertiesMetricEnglishComments
Melt Temperature 275 °C527 °FInjection molding
Mold Temperature 115 °C239 °FInjection molding
 
Descriptive Properties
ColorBK-112
Commercial StatusActive America
FormPellets
Impact ModifiedNo
Primary Processing TechniqueInjection Molding
ProcessingInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Petra® 130 FR 30% Glass Filled PET
Dow DNDA-7144 NT 7 Linear Low Density Polyethylene Resin
Lavergne VYPET VNT 635A PET 35% Glass Reinforced
MOCOM (ALBIS) Tedur® P 9519 PPS, ~45% Glass Fiber (black only)
Overview of materials for PVC, High Impact

PBASF9021 / 84785

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.