MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Chevron Phillips Marlex® D174 Polyethylene Film Grade LLDPE Hexene Copolymer
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Film Grade; LLDPE/Hexene, Film Grade

Material Notes: This metallocene linear low density polyethylene is an ethylene-hexene copolymer tailored for cast film applications that require: • Superior clarity • Excellent gloss • Exceptional toughness• Outstanding heat seal.

Typical cast film applications include: • Stretch wrap • Overwrap • Co extrusions.

information provided by Chevron Phillips Chemical Company LP.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.918 g/cc0.0332 lb/in³ASTM D1505
Thickness 25.4 microns1.00 milAs Tested
Melt Flow 4.5 g/10 min
@Load 2.16 kg,
Temperature 190 °C
4.5 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Antiblock Level 0.000 ppm0.000 ppm
Slip Level 0.000 ppm0.000 ppm
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 10.0 MPa
@Thickness 0.0254 mm
1450 psi
@Thickness 0.00100 in
ASTM D882
Film Tensile Strength at Yield, TD 9.00 MPa
@Thickness 0.0254 mm
1310 psi
@Thickness 0.00100 in
ASTM D882
Film Elongation at Break, MD 550 %
@Thickness 0.0254 mm
550 %
@Thickness 0.00100 in
ASTM D882
Film Elongation at Break, TD 680 %
@Thickness 0.0254 mm
680 %
@Thickness 0.00100 in
ASTM D882
Coefficient of Friction >= 1.0>= 1.0ASTM D1894
Elmendorf Tear Strength MD 300 g
@Thickness 0.0254 mm
300 g
@Thickness 0.00100 in
ASTM D1922
Elmendorf Tear Strength TD 500 g
@Thickness 0.0254 mm
500 g
@Thickness 0.00100 in
ASTM D1922
Elmendorf Tear Strength, MD 11.8 g/micron
@Thickness 0.0254 mm
300 g/mil
@Thickness 0.00100 in
ASTM D1922
Elmendorf Tear Strength, TD 19.7 g/micron
@Thickness 0.0254 mm
500 g/mil
@Thickness 0.00100 in
ASTM D1922
Dart Drop 10.2 g/micron
@Thickness 0.0254 mm
260 g/mil
@Thickness 0.00100 in
ASTM D1709
Dart Drop Test 260 g
@Thickness 0.0254 mm
0.573 lb
@Thickness 0.00100 in
ASTM D1709
Film Tensile Strength at Break, MD 54.0 MPa
@Thickness 0.0254 mm
7830 psi
@Thickness 0.00100 in
ASTM D882
Film Tensile Strength at Break, TD 47.0 MPa
@Thickness 0.0254 mm
6820 psi
@Thickness 0.00100 in
ASTM D882
1% Secant Modulus, MD 110 MPa
@Thickness 0.0254 mm
16000 psi
@Thickness 0.00100 in
ASTM D882
1% Secant Modulus, TD 117 MPa
@Thickness 0.0254 mm
17000 psi
@Thickness 0.00100 in
ASTM D882
Heat Seal Strength Initiation Temperature 101 °C214 °F0.3 lb/in heat seal strength achieved. 0.5 s dwell, 30 psi pressure, 11.8 in/min separation rate.; ASTM F88
 
Optical PropertiesMetricEnglishComments
Haze 2.0 %
@Thickness 0.0254 mm
2.0 %
@Thickness 0.00100 in
ASTM D1003
Gloss 140 %
@Thickness 0.0254 mm
140 %
@Thickness 0.00100 in
60°; ASTM D2457
 
Descriptive Properties
Process Aidnone

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCHEVC8914 / 241997

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.