MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

European Scots Pine Wood
Categories: Wood and Natural Products; Wood; Softwood

Material Notes: Data is based on small, clear, air-dried samples unless specified.
Usual surface texture: Coarse
Dimensional changes when dried lumber is subjected to variations in humidity during service: Medium
Resistance to fungal decay (Heartwood in ground contact): Non-durable (5 to 10 years)
Resistance to penetration by preservatives: Moderately resistant
Common Applications: Construction, joinery

Key Words: Pinus sylvestris; Lumber, Timber
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.360 g/cc0.0130 lb/in³Earlywood
 0.730 g/cc0.0264 lb/in³Latewood
Cell Length 3.10 mm0.122 inMature Wood
 
Mechanical PropertiesMetricEnglishComments
Hardness, Wood Indentation 2400 N540 lb (f)Side
Tensile Strength, Ultimate 2.90 MPa421 psiPerpendicular to Grain
 102 MPa14800 psiAxial
Modulus of Rupture 0.0980 GPa14.2 ksiStatic Bending
Flexural Modulus 11.76 GPa1706 ksiStatic Bending
Compressive Strength 7.50 MPa1090 psiPerpendicular to Grain
 54.0 MPa7830 psiParallel to Grain
Machinability 50 %50 %Medium Relative to Other Wood
Shear Strength 9.80 MPa1420 psiOrientation Unknown
Toughness 27.6 J20.4 ft-lb2 cm x 2 cm sample
Cleavage 3.60 kN/m20.5 lb/in
 
Thermal PropertiesMetricEnglishComments
Shrinkage 0.40 %0.40 %Axial; Green to Zero Moisture
 1.0 %1.0 %Radial; Green to Zero Moisture
 7.7 %7.7 %Tangential; Green to Zero Moisture
 12.4 %12.4 %Volumetric; Green to Zero Moisture
 
Descriptive Properties
ColorPale yellowish-brown to red-brownUsual for heartwood

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
American Pine Wood
Northern White Pine Wood
Southern Pine Wood
European Umbrella Pine (Parasol Pine, Stone Pine) Wood
Lodgepole Pine Wood

PTSE550 / 71329

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.