MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Akro-Plastic Akroloy® PA GF 60 natural (2941) PA 66 + PA 6I/6T Conditioned, 60% Glass Filled
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 60% Glass Fiber Filled

Material Notes: Description: Akroloy PA GF 60 natural (2941) is a 60% glass fiber reinforced polyamide blend with very high stiffness and strength, even in conditioned state. This material is listed at UL at 0.8 mm all colors HB. Applications are components with high dimensional stability, independent from moisture content. Akroloy PA GF 60 is an alternative for aluminum and zinc diecast alloys.

Features:

  • Good Dimensional Stability
  • High Stiffness
  • High Strength
Uses: Metal Replacement

Information provided by Akro-Plastic GmbH

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.72 g/cc0.0621 lb/in³ISO 1183
Filler Content 60 %60 %ISO 1172
Moisture Absorption 0.80 %
@Temperature 70.0 °C
0.80 %
@Temperature 158 °F
Humidity, 62% RH; ISO 1110
Water Absorption at Saturation 3.0 - 3.5 %3.0 - 3.5 %ISO 62
Linear Mold Shrinkage, Flow <= 0.0030 cm/cm<= 0.0030 in/inISO 294-4
Linear Mold Shrinkage, Transverse 0.0050 cm/cm0.0050 in/inISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 245 MPa35500 psi5 [mm/min]; ISO 527-2
Elongation at Break 2.5 %2.5 %5 [mm/min]; ISO 527-2
Tensile Modulus 20.0 GPa2900 ksi1 [mm/min]; ISO 527-2
Charpy Impact Unnotched 9.50 J/cm²
@Temperature 23.0 °C
45.2 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched 1.60 J/cm²
@Temperature 23.0 °C
7.61 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Melting Point 255 °C491 °FDIN EN 11357-1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Akro-Plastic Akroloy® PA GF 50 (2706) PA 6.6 & PA6I/6T Dry, 50% Glass Filled
Akro-Plastic Akroloy® PA GF 60 natural (2941) PA 66 + PA 6I/6T Dry, 60% Glass Filled
Akro-Plastic Akroloy® PA GF 60 (2844) PA 6.6 & PA6I/6T Dry, 60% Glass Filled
Lubrizol Isoplast® 101LGF60NAT Engineering Thermoplastic Polyurethane Resin
Lubrizol Isoplast® 101LGF40NAT Engineering Thermoplastic Polyurethane Resin

PAKRO108 / 182695

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.