MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

ATI Allegheny Ludlum Grade 18 Titanium (UNS R56322)
Categories: Metal; Nonferrous Metal; Titanium Alloy; Alpha/Near Alpha Titanium Alloy

Material Notes: Uses: heat exchangers, industrial components, tubing.

Mechanical property data below is typical of annealed samples at room temperature.

Information provided by Allegheny Ludlum.

Key Words: ASTM B-265
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 4.52 g/cc0.163 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell C 2525
Tensile Strength, Ultimate 760 MPa110000 psi
Tensile Strength, Yield 655 MPa
@Strain 0.2 %
95000 psi
@Strain 0.2 %
Elongation at Break 15 %15 %
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 3.0 %3.0 %
Carbon, C <= 0.050 %<= 0.050 %
Hydrogen, H <= 0.015 %<= 0.015 %
Iron, Fe <= 0.13 %<= 0.13 %
Nitrogen, N <= 0.010 %<= 0.010 %
Oxygen, O <= 0.10 %<= 0.10 %
Palladium, Pd 0.050 %0.050 %
Titanium, Ti 94.5 %94.5 %as balance
Vanadium, V 2.5 %2.5 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Titanium Ti-6Al-4V (Grade 5), Annealed
ATI Allvac® 6-2-4-6 Titanium Alloy, Heat Treatment: 885°C (1625°F) + Age
ATI Allvac® Ti-17 Titanium Alloy, Heat Treatment: 899°C (1650°F) + Age
ATI Allegheny Ludlum Grade 23 (6-4 ELI) Titanium (UNS R56401)
Titanium Grade 18 Ti-3Al-2.5V-0.05Pd

NLTIT18 / 18063

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.