MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Aremco

Aremco HiE-Coat™ 840-MX High Emissivity Coating, Inorganic-Ceramic Filled
Categories: Ceramic; Other Engineering Material; Ceramic/Metallic Coating

Material Notes: Ceramic-based, black pigmented coating for carbon and stainless steel to 2400 ºF (1316 ºC). Aremco’s HiE-Coat™ 840-Series line of high emissivity coatings are black-body formulations designed to significantly improve the thermal efficiency of infrared heaters, furnaces, incinerators, and ovens used throughout the appliance, ceramics, chemical processing, metallurgical, and refining industries.

Vendors: Aremco’s HiE-Coat line of high emissivity coatings are black-body systems formulated to significantly improve the thermal efficient of infrared heaters, heat exchangers and furnaces for applications to 2500°F (1371°C). Visit us today at Aremco.com or call 1 (845) 268-0039 to speak with an engineer.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.57 g/cc0.0567 lb/in³
Solids Content 22.1 %22.1 %by volume
 47.3 %47.3 %by weight
Volatile Organic Compounds (VOC) Content 0.00 g/l0.00 g/l
Viscosity 300 - 700 cP300 - 700 cP
Thickness 25.4 microns1.00 milrecommended dry film thickness
 115 microns4.52 milestimated wet film thickness
Storage Temperature 12.8 - 29.4 °C55.0 - 85.0 °F
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 1320 °C2400 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature 50.0 - 90.0 °C122 - 194 °FApplication Temp
Cure Time  60.0 min
@Temperature 93.3 °C
1.00 hour
@Temperature 200 °F
Step 1, preceded by 1 hour air set
 60.0 min
@Temperature 260 °C
1.00 hour
@Temperature 500 °F
Step 2
Shelf Life 6.00 Month
@Temperature 12.8 - 29.4 °C
6.00 Month
@Temperature 55.0 - 85.0 °F
 
Descriptive Properties
ColorJet Black
Dry Film Coverage ft2/gal355at 1 mil
Thinner840-MX-T

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

CAREM41m / 256038

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.