MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Arla MAKROTECH™ UV PC Sheet
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Extruded

Material Notes: Arla Plast MAKROTECH™ UV is a range of opaque colored polycarbonate sheets. The product is virtually unbreakable with extremely high impact resistance. The product offers high temperature performance too. MAKROTECH™ UV is one side UV-protected sheet which allows possibilities for outdoor applications.

Also Available: Two side UV protection; With stripe applied for identification in packaging industry; MAKROTECH™ CC for metallic colors; MAKROTECH™ ECC for extra depth in metallic colors
Recycling: The total recycling concept (TRC) covers all types of sheets to provide cost savings. Off-cuts from the sheets can be used in production of new sheets by co-extruding virgin material as the top layer. Care is taken that all quality requirements are met.

Benefits: UV protected topside; Unique metallic colors; High impact strength; Wide temperature range

Application: Outdoor flat, curved and formed parts for applications in automotive, agricultural, covers and containers, wall cladding, signage.

Information provided by Arla Plast.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.20 g/cc0.0434 lb/in³ISO 1183
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 7070ISO 2039-2
Tensile Strength, Yield 60.0 MPa8700 psiISO 527
Modulus of Elasticity 2.30 GPa334 ksiISO 527
Flexural Strength >= 90.0 MPa>= 13100 psiISO 178
Flexural Modulus 2.30 GPa334 ksiISO 178
Izod Impact, Notched (ISO) 65.0 kJ/m²30.9 ft-lb/in²ISO 180
Izod Impact, Unnotched (ISO) NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 180/1U
 10.0 kJ/m²
@Thickness 4.00 mm,
Temperature -30.0 °C
4.76 ft-lb/in²
@Thickness 0.157 in,
Temperature -22.0 °F
ISO 180/1U
 
Thermal PropertiesMetricEnglishComments
CTE, linear 70.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
38.9 µin/in-°F
@Temperature 73.4 - 176 °F
Deflection Temperature at 1.8 MPa (264 psi) 132 °C270 °FISO 75
Vicat Softening Point 149 °C300 °FB120; ISO 306
Flammability, UL94 HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PARLA911 / 301089

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.