MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

American Eastern White Pine Wood
Categories: Wood and Natural Products; Wood; Softwood

Material Notes: Softwood. Easy to work with hand tools. Data is based on small, clear, air-dried samples unless specified.

Key Words: Pinus strobus; Lumber, Timber
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.350 g/cc0.0126 lb/in³Air Dry (12-15% Moisture Content)
Cell Length 3.00 mm0.118 inMature Wood
 
Mechanical PropertiesMetricEnglishComments
Hardness, Wood Indentation 1700 N382 lb (f)Side
Tensile Strength, Ultimate 2.10 MPa305 psiPerpendicular to Grain
 78.0 MPa11300 psiAxial
Modulus of Rupture 0.0590 GPa8.56 ksiIn Bending
Flexural Yield Strength 41.4 MPa6000 psiBending stress at proportional limit
Flexural Modulus 8.30 - 8.56 GPa1200 - 1240 ksiIn Bending
Compressive Strength 3.50 MPa508 psiPerpendicular to Grain
 33.0 - 33.1 MPa4790 - 4800 psiParallel to Grain
Shear Strength 6.20 MPa899 psiOrientation Unknown
Toughness 12.4 J9.15 ft-lbRadial
 13.6 J10.0 ft-lbTangential
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 0.0908 W/m-K0.630 BTU-in/hr-ft²-°FOven Dry
 0.108 W/m-K0.750 BTU-in/hr-ft²-°F12% Moisture Content
Shrinkage 2.3 %2.3 %Radial; Green to Zero Moisture
 6.0 %6.0 %Tangential; Green to Zero Moisture
 8.2 %8.2 %Volumetric; Green to Zero Moisture

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
American Pine Wood
Northern White Pine Wood
Southern Pine Wood
American Ponderosa Pine Wood
North American Loblolly Pine Wood

PTSAH / 71291

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.