Borecene Compact RM8406 is a third generation linear medium density black polyethylene for rotational molding. The narrow molecular weight imparted through metallocene catalyst technology provides an ideal balance of flow and physical properties. Borecene Compact RM8406 is a black version of Borecene RM8403, suitable for diesel fuel tanks. Borecene Compact RM8406 is delivered as new technology powder. Information provided by the Manufacturer. |