MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

DuPont Nucrel® 0609HS Ethylene-Methacrylic Acid Copolymer Resin for Extrusion Coating/Laminating  (discontinued **)
Categories: Polymer; Thermoplastic; Ethylene Methyl Acrylate; Ethylene-Methyl Acrylate Copolymer, Coating Grade

Material Notes: 6 wt% Methacrylic Acid.

Nucrel® 0609HS* (High-Speed) is an ethylene-methacrylic acid copolymer resin available for use in conventional extrusion coating, coextrusion coating, and extrusion laminating equipment designed to process polyethylene resins. Formerly Nucrel® RX3993-1.

Features/Benefits vs. Nucrel® 0411HS: Better adhesion to unprimed foil, paper and metallized film provides better substrate protection, improved structure reliability, and barrier integrity. This product provides good, but lower adhesion to PE. Lower seal initiation temperature allows higher speed packaging. Better hot tack, sealability through contamination and heat seal strength provides stronger, more reliable heat seals.

Typical Applications: Foil-containing shampoo, toothpaste, towelette, condiment and miscellaneous non-food pouches and sachets; Medical/pharmaceutical packaging Snack structures; Toothpaste tubes; Aseptic and hot-fill liquid cartons; Other foil, metallized film, or paper coatings as a heat seal or tie layer.

Information provided by DuPont Packaging Polymers.

This product line/trade name was acquired by Dow, but this specific grade was discontinued prior to the acquisition.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Melt Flow 9.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
9.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Seal Strength 2800 g/25 mm2800 g/inseal bar 125°C.
Hot Tack Strength 700 g/25 mm700 g/inseal bar 115°C; Packforsk method.
 
Thermal PropertiesMetricEnglishComments
Melting Point 83.0 °C181 °FFreezing Point via DSC/ASTM D3418
 104 °C219 °FUpon Melting via DSC/ASTM D3418
Vicat Softening Point 88.0 °C190 °FASTM D1525
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 305 °C581 °FTypical Die Temp.
Melt Temperature 260 - 315 °C500 - 599 °Fflat die equipment

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow Nucrel® 0411HS Ethylene-Methacrylic Acid Copolymer Resin for Extrusion Coating/Laminating
DuPont Elvaloy® 1126 AC Ethylene and 25% Methyl Acrylate Copolymer
Dow Nucrel® 0609HSA Ethylene-Methacrylic Acid Copolymer Resin for Film and Extrusion Coating/Laminating
Dow Nucrel® 0908HS Ethylene-Methacrylic Acid Copolymer Resin for Film and Extrusion Coating/Laminating
Dow Nucrel® 903 Ethylene-Methacrylic Acid Copolymer Resin for Blown and Cast Film

PDUPJ3 / 33637

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.