MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Sandvik Osprey 17-4 PH Stainless Steel Powder (Grade 90% - 22)
Categories: Metal; Ferrous Metal; Stainless Steel; Precipitation Hardening Stainless

Material Notes: Particle size distribution 1-250 microns. Typical distribution:
  • 90% < 22 microns
  • 80% < 16 microns
  • 52% < 10 microns
  • 15% < 5 microns
Mean size is 10.0  microns.

Material Notes: Composition above is typical of 17-4 PH precipitation hardening stainless. This alloy is widely used because of its high strength, high hardness, excellent corrosion resistance, and easy heat treatment. The 17-4 PH alloy is used in aerospace, medical, food processing, and chemical industries for applications such as pump shafts, valve stems, braces, fasteners, coupling, rocket and missile components, hydraulic actuators, and wear rings. SHAPE: Predominantly spherical PACKAGING: 4 & 20 Kg. Chemical composition and particle size distribution can be adjusted to suit customers' requirements.

The specifications listed are subject to the benefits and scrutiny of Osprey's accreditation to ISO 9001.

Information provided to MatWeb by Osprey Metals, now Sandvik Osprey Ltd.

Key Words: UNS S17400, Powder Metallurgy, Metal Powder, Metal Injection Molding, MIM, Microfine, 17-4PH, 17/4PH, 17-4 PH, 17/4PH, Precipitation Hardening
Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Particle Size 10 µm10 µmMean
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.010 %0.010 %Typical
 <= 0.070 %<= 0.070 %
Chromium, Cr 15.5 - 17.5 %15.5 - 17.5 %
Copper, Cu 3.0 - 5.0 %3.0 - 5.0 %
Iron, Fe 71.85 %71.85 %As Balance
Manganese, Mn 0.76 %0.76 %Typical
 <= 1.0 %<= 1.0 %
Molybdenum, Mo <= 0.30 %<= 0.30 %
Nickel, Ni 3.0 - 5.0 %3.0 - 5.0 %
Niobium, Nb (Columbium, Cb) 0.15 - 0.45 %0.15 - 0.45 %
Phosphorus, P <= 0.040 %<= 0.040 %
Silicon, Si 0.84 %0.84 %Typical
 <= 1.0 %<= 1.0 %
Sulfur, S <= 0.030 %<= 0.030 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ametek 17-4 P/M Process, Sintered at 2200°F (1204°C)
Sandvik Osprey 17-4 PH Stainless Steel Powder (Grade 95% - 16)
FloMet 17-4 PH Stainless Steel, As Sintered
Kinetics MIM 17-4PH Stainless Steel (H900 Condition)
Sandvik Osprey 17-4 PH Stainless Steel Powder (Grade 90% - 16)

NOSPR013 / 18535

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.