MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Flame Retardant adhesives

Sumitomo Bakelite Sumikon® PM-6545 Phenolic Resol
Categories: Polymer; Thermoset; Phenolic; Phenolic, Novolac, Mineral/Glass Filled

Material Notes: SUMIKON® PM-6545 type black is a glass fiber filled resol resin molding compound with good mechanical properties and heat resistance. This grade suits UL1004.

Information provided by Sumitomo Bakelite High Performance Plastics (sbhpp)

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.99 g/cc1.99 g/ccJIS K 6911
Water Absorption 0.11 %0.11 %JIS K 6911
Linear Mold Shrinkage 0.0019 cm/cm0.0019 in/inJIS K 6911
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 94.0 MPa13600 psiJIS K 6911
Flexural Strength 176 MPa25500 psiJIS K 6911
Flexural Modulus 20.9 GPa3030 ksiJIS K 6911
Compressive Strength 145 MPa21000 psiJIS K 6911
Charpy Impact, Notched 0.380 J/cm²1.81 ft-lb/in²JIS K 6911
 
Electrical PropertiesMetricEnglishComments
Insulation Resistance 8.00e+11 ohm8.00e+11 ohmAfter boiling; JIS K 6911
 7.00e+12 ohm7.00e+12 ohmAs mold; JIS K 6911
Dielectric Strength 12.0 kV/mm305 kV/inJIS K 6911
Comparative Tracking Index 250 V250 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 300 °C572 °FJIS K 6911
Flammability, UL94 V-0V-0
 
Descriptive Properties
ColorBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Sumitomo Bakelite Durez® 152 Phenolic, Compression Grade
Sumitomo Bakelite Durez® 118 Phenolic, Injection Grade
Sumitomo Bakelite Durez® 118 Phenolic, Compression Grade
Bakelite® PF 1110 Phenolic Molding Compound

PSUMIT454 / 194259

Flame Retardant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.