MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Angst+Pfister APSOplast® PUR D15 95 Sh. A Polyester urethane (AU)
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Chemically, PUR D15 is based on polyester polyol + naphthylene-1.5-diisocyanate (DESMODUR® 15). PUR D15 is a high-quality polyurethane with unsurpassed abrasion and structural strength; however, it is not stable when exposed to hydrolysis. In comparison with other PUR elastomers, PUR D15 has increased resistance to heat. Short-term exposure to temperatures of up to +120 °C are possible. However, the material should not be exposed to a long-term temperature of over +100 °C. A further advantage of PUR D15 is that it has a higher modulus of elasticity in comparison with other PUR elastomers of the same Shore hardness, and thus has a higher load-bearing capacity while retaining the same deformation values. The hardness of PUR D15 is between approx. 65 Shore A to 70 Shore D.

Information provided by Angst + Pfister

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 9595DIN 53505
Tensile Strength at Break 35.0 MPa5080 psiDIN 53504
Tensile Stress at Strain  10.6 MPa
@Strain 100 %
1540 psi
@Strain 100 %
DIN 53504
 15.8 MPa
@Strain 300 %
2290 psi
@Strain 300 %
DIN 53504
Elongation at Break 702 %702 %DIN 53504
Rebound 61 %61 %DIN 53512
Tear Strength 57.0 kN/m325 pliDIN 53515
Abrasion 2626[mm3]; DIN 53516
Compression Set  13 %
@Temperature 23.0 °C,
Time 252000 sec
13 %
@Temperature 73.4 °F,
Time 70.0 hour
DIN 53517
 21 %
@Temperature 70.0 °C,
Time 86400 sec
21 %
@Temperature 158 °F,
Time 24.0 hour
DIN 53517

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PANGP108 / 250606

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.