MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Beryllium-Copper Casting Alloy 275C, UNS C82800, TF00 Temper
Categories: Metal; Nonferrous Metal; Copper Alloy; Copper Casting Alloy

Material Notes:

Casting methods recommended for this alloy: Centrifugal, Investment, Permanent Mold, Plaster, and Sand.

Applications: Bearings and molds for plastic parts.

Test specimen: TF00 temper, solution treated at 790-800°C, aged 3 hours at 3

Key Words: BeCu; beryllium copper 275C, CA 828, FED QQ-C-390, MIL-T-16243, MIL-C-19464 (Class IV), ICI-Cu-2-10789
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.09 g/cc0.292 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell A  30
@Temperature 500 °C
30
@Temperature 932 °F
hot hardness
 60
@Temperature 400 °C
60
@Temperature 752 °F
hot hardness
 70
@Temperature 300 °C
70
@Temperature 572 °F
hot hardness
 73
@Temperature 200 °C
73
@Temperature 392 °F
hot hardness
 74
@Temperature 30.0 °C
74
@Temperature 86.0 °F
hot hardness
 74
@Temperature 100 °C
74
@Temperature 212 °F
hot hardness
Hardness, Rockwell C 4646
Tensile Strength, Ultimate 1140 MPa165000 psi
 565 MPa
@Temperature 425 °C
81900 psi
@Temperature 797 °F
 595 MPa
@Temperature 400 °C
86300 psi
@Temperature 752 °F
 970 MPa
@Temperature 300 °C
141000 psi
@Temperature 572 °F
 1220 MPa
@Temperature 200 °C
177000 psi
@Temperature 392 °F
 1275 MPa
@Temperature 20.0 °C
184900 psi
@Temperature 68.0 °F
 1280 MPa
@Temperature 100 °C
186000 psi
@Temperature 212 °F
Tensile Strength, Yield 1070 MPa
@Strain 0.2 %
155000 psi
@Strain 0.2 %
Elongation at Break 1.0 %1.0 %In 50 mm
 0.60 %
@Temperature 300 °C
0.60 %
@Temperature 572 °F
 1.1 %
@Temperature 200 °C
1.1 %
@Temperature 392 °F
 1.4 %
@Temperature 100 °C
1.4 %
@Temperature 212 °F
 1.6 %
@Temperature 0.000 °C
1.6 %
@Temperature 32.0 °F
 2.3 %
@Temperature 400 °C
2.3 %
@Temperature 752 °F
 2.8 %
@Temperature 460 °C
2.8 %
@Temperature 860 °F
Modulus of Elasticity 133 GPa19300 ksi
Poissons Ratio 0.300.30
Machinability 10 - 20 %10 - 20 %UNS C36000 (free-cutting brass) = 100%
Shear Modulus 51.0 GPa7400 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000958 ohm-cm
@Temperature 20.0 °C
0.0000958 ohm-cm
@Temperature 68.0 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear 17.0 µm/m-°C
@Temperature 20.0 - 200 °C
9.44 µin/in-°F
@Temperature 68.0 - 392 °F
Specific Heat Capacity 0.420 J/g-°C0.100 BTU/lb-°F
Thermal Conductivity 95.0 W/m-K
@Temperature 20.0 °C
659 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
Melting Point 855 °C1570 °FIncipient
 860 - 930 °C1580 - 1710 °F
Solidus 835 °C1540 °F
Liquidus 930 °C1710 °F
Shrinkage 1.56 %1.56 %Patternmaker's Shrinkage (3/16 in./ft.)
 
Processing PropertiesMetricEnglishComments
Solution Temperature 790 - 800 °C1450 - 1470 °F
Aging Temperature 345 °C653 °F
Casting Temperature 965 - 1040 °C1770 - 1900 °FHeavy castings
 1040 - 1150 °C1900 - 2100 °FLight castings
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al <= 0.15 %<= 0.15 %
Beryllium, Be 2.5 - 2.75 %2.5 - 2.75 %
Chromium, Cr <= 0.10 %<= 0.10 %
Cobalt, Co 0.37 - 0.70 %0.37 - 0.70 %
Copper, Cu >= 94.8 %>= 94.8 %
Iron, Fe <= 0.25 %<= 0.25 %
Lead, Pb <= 0.020 %<= 0.020 %
Nickel, Ni <= 0.20 %<= 0.20 %
Silicon, Si 0.20 - 0.35 %0.20 - 0.35 %
Tin, Sn <= 0.10 %<= 0.10 %
Zinc, Zn <= 0.10 %<= 0.10 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Beryllium-Copper Casting Alloy 275C, UNS C82800, Cast and Aged
Beryllium-Copper Casting Alloy 275C, UNS C82800, TB00 Temper
Leaded Semi-Red Brass, UNS C84800, Copper Casting Alloy
Beryllium-Copper Casting Alloy 275C, UNS C82800, As-Cast
Beryllium Copper 21C UNS C82510 Casting Alloy Solution Treated and Aged

MC82800b5 / 11898

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.