System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Conventus Polymers Duramide™ PA66LGF60BK Nylon 66, 60% Long Glass Fiber Reinforced, Heat Stabilized
Categories:
Polymer
;
Thermoplastic
;
Nylon (Polyamide PA)
;
Nylon 66 (PA66)
;
Nylon 66, 60% Glass Fiber Filled
Material Notes:
Duramide PA66LGF60BK is a 60% long glass fiber, heat stabilized Nylon 66 compound using pultrusion method. It is available in US, Europe, and Asia. Black in color.
Information provided by Conventus Polymers.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Specific Gravity
1.69
g/cc
1.69
g/cc
ASTM D792
Mechanical Properties
Metric
English
Comments
Tensile Strength at Break
261
MPa
37900
psi
ASTM D638
Elongation at Break
2.0 %
2.0 %
ASTM D638
Tensile Modulus
20.0
GPa
2900
ksi
ASTM D638
Flexural Strength
405
MPa
58800
psi
ASTM D790
Flexural Modulus
16.5
GPa
2400
ksi
ASTM D790
Izod Impact, Notched
5.18
J/cm
9.70
ft-lb/in
ASTM D256
Izod Impact, Unnotched
14.4
J/cm
27.0
ft-lb/in
ASTM D4812
Thermal Properties
Metric
English
Comments
Deflection Temperature at 1.8 MPa (264 psi)
243
°C
470
°F
ASTM D648
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
PCONV922 / 233822
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.