MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Borealis Visico™/Ambicat™ ME4425/LE4472 Ambient Curing, Moisture-Crosslinking Polyethylene Compound for Low Voltage Insulation
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Wire/Cable Grade

Material Notes: Visico LE4423 is a natural, ethylene vinyl silane copolymer that, when combined with the catalyst masterbatch Ambicat LE4472, will undergo an accelerated, moisture-induced crosslinking reaction. This polyethylene compound is highly active and crosslinks rapidly under ambient temperature and humidity conditions, as well as, in a sauna or hot water bath. The combinations of the Visico medium-density polyethylene base material, ME4425, and the patented sulphonic acid catalyst masterbatch, LE4472, provides a highly scorch retardant compound with excellent thermal stability. The higher density of ME4425 exhibits greater chemical resistance, toughness and improved heat deformation resistance. ME4425 contains a permanent scorch retardant additive (SRA) that increases the processing window for moisture crosslinking compound, minimizes the tendency for premature crosslinking in the extruder, head or die and allows the use of highly active crosslinking catalyst like LE4472. LE4472 should be added to ME4425 directly in the extruder hopper by dry blending at a ratio of 7 parts LE4472 to 93 parts ME4425.

Information provided by the Manufacturer.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.930 g/cc0.0336 lb/in³Base ME 4425; ASTM D792
 1.38 g/cc0.0499 lb/in³Catalyst LE 4472; ASTM D792
Melt Index of Compound 0.70 g/10 min0.70 g/10 minME 4425; ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield >= 18.6 MPa>= 2700 psiHeat Aging (7 Days at 121°C); ASTM D412
 20.7 MPa3000 psiASTM D412
Elongation at Break >= 315 %>= 315 %Heat Aging (7 Days at 121°C); ASTM D412
 350 %350 %ASTM D412
Elongation at Yield >= 50 %>= 50 %Hot Creep Test (150°C, 0.20 MPa); ICEA T-28-562
Tensile Set <= 5.0 %<= 5.0 %Hot Creep Test (150°C, 0.20 MPa); ICEA T-28-562
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.00e+16 ohm-cm1.00e+16 ohm-cmASTM D257
Dielectric Constant 2.3
@Frequency 60 Hz
2.3
@Frequency 60 Hz
ASTM D150
Dielectric Strength >= 21.7 kV/mm>= 550 kV/inASTM D149
Dissipation Factor 0.00050
@Frequency 60 Hz
0.00050
@Frequency 60 Hz
ASTM D150

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Low Density Polyethylene (LDPE), Molded
Overview of materials for Polyester Thermoplastic Elastomer
Overview of materials for Low Density Polyethylene (LDPE), Masterbatch Grade
Overview of materials for Low Density Polyethylene (LDPE), Film Grade
Overview of materials for Low Density Polyethylene (LDPE), Extrusion Grade

PBOREA006 / 27313

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.