MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Chase Electronic Coatings HumiSeal® 1100 Stripper
Categories: Fluid; Solvent

Material Notes: HumiSeal® Stripper 1100 removes dual cure acrylated urethane conformal coatings such as UV40 family products. HumiSeal® Stripper 1100 does not contain any halogenated hydrocarbons, aromatics or flammable ingredients. Unlike methylene chloride based products that evaporated quickly, HumiSeal® Stripper 1100 remains on the surface to penetrate and soften the coating. HumiSeal® Stripper 1100 will not remove or attack solder, copper, silver, gold and nickel plating. HumiSeal® Stripper 1100 is in full compliance with the RoHS Directive (Directive 2002/95/EC).

Information provided by Chase Electronic Coatings.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.05 g/cc0.0379 lb/in³
Volatile Organic Compounds (VOC) Content 1.049 g/l1.049 g/l
 
Thermal PropertiesMetricEnglishComments
Flash Point 92.8 °C199 °FTCC
 
Processing PropertiesMetricEnglishComments
Shelf Life 36.0 Month36.0 MonthDOM
 
Descriptive Properties
Colorlight amber to clear
Relative Evaporating Rate<1.0BuAc = 1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCHAS938 / 239799

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.