MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Avient Edgetek® CY-20GF/000 UV FR V0 PC/ABS Blend, Glass Filled  (discontinued **)
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Glass Fiber Filled; Polycarbonate (PC)

Material Notes:

Description/Features:

  • Glass Fiber Reinforced
  • Ignition Resistant
  • Non-Halogenated
PolyOne First Choice

Information provided by PolyOne Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.29 g/cc1.29 g/ccASTM D792
Linear Mold Shrinkage 0.0070 cm/cm0.0070 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 64.8 MPa9400 psiType 1 - Rigids, 0.2 in/min; ASTM D638
Elongation at Break 0.60 %0.60 %Type 1 - Rigids, 0.2 in/min; ASTM D638
Tensile Modulus 13.02 GPa1888 ksiType 1 - Rigids, 0.2 in/min; ASTM D638
Flexural Strength 100 MPa14500 psiASTM D790
Flexural Modulus 10.3 GPa1500 ksiASTM D790
Izod Impact, Notched 0.278 J/cm
@Thickness 6.35 mm,
Temperature 23.0 °C
0.520 ft-lb/in
@Thickness 0.250 in,
Temperature 73.4 °F
Method A, Injection Molded; ASTM D256
 
Thermal PropertiesMetricEnglishComments
Flammability, UL94 V-0
@Thickness 3.17 mm
V-0
@Thickness 0.125 in
All Colors
 
Processing PropertiesMetricEnglishComments
Melt Temperature 232 - 260 °C450 - 500 °FMolding
Mold Temperature 82.2 - 93.3 °C180 - 200 °F
Drying Temperature 93.3 °C200 °F
Dry Time 4 hour4 hour
 
Descriptive Properties
Product FormPellets

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Versalis KOBLEND PCA PD 935 G2 PC+ABS, 10% Glass Fiber
Avient Edgetek® CY-10GF/000 UV FR V0 NATURAL PC/ABS Blend, Glass Filled
Mocom (ALBIS) ALCOM® PC+ABS 750/10 GF10 RD1016-05LB PC+ABS, 10% Glass Fiber Reinforced
Covestro Bayblend® T88-4N Polycarbonate + ABS, 20% Glass Filled
Geon® Performance Solutions 92052 Exterior Extrusion PVC

PH1PO0260 / 43453

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.