MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Silver-Magnesium-Nickel Alloy (Ag-0.25Ni-0.25Mg), Oxidized
Categories: Metal; Nonferrous Metal; Precious Metal; Silver Alloy

Material Notes: This alloy can be strengthened by oxidation, typically after fabrication. The Mg oxidizes and creates tiny MgO particles to provide dispersion strengthening.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 10.49 g/cc0.3790 lb/in³(pure silver)
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate  >= 385 MPa
@Thickness 12.2 - 15.5 mm
>= 55800 psi
@Thickness 0.480 - 0.610 in
 >= 400 MPa
@Thickness 7.62 - 11.4 mm
>= 58000 psi
@Thickness 0.300 - 0.450 in
 >= 415 MPa
@Thickness 4.57 - 6.35 mm
>= 60200 psi
@Thickness 0.180 - 0.250 in
 >= 425 MPa
@Thickness 3.81 mm
>= 61600 psi
@Thickness 0.150 in
Tensile Strength, Yield  >= 325 MPa
@Strain 0.2 %,
Thickness 12.2 - 15.5 mm
>= 47100 psi
@Strain 0.2 %,
Thickness 0.480 - 0.610 in
 >= 340 MPa
@Strain 0.2 %,
Thickness 7.62 - 11.4 mm
>= 49300 psi
@Strain 0.2 %,
Thickness 0.300 - 0.450 in
 >= 360 MPa
@Strain 0.2 %,
Thickness 4.57 - 6.35 mm
>= 52200 psi
@Strain 0.2 %,
Thickness 0.180 - 0.250 in
 >= 380 MPa
@Strain 0.2 %,
Thickness 3.81 mm
>= 55100 psi
@Strain 0.2 %,
Thickness 0.150 in
Elongation at Break  >= 9.0 %
@Thickness 3.81 mm
>= 9.0 %
@Thickness 0.150 in
in 2 in. (50 mm)
 >= 12 %
@Thickness 4.57 - 6.35 mm
>= 12 %
@Thickness 0.180 - 0.250 in
in 2 in. (50 mm)
 >= 13 %
@Thickness 7.62 - 11.4 mm
>= 13 %
@Thickness 0.300 - 0.450 in
in 2 in. (50 mm)
 >= 14 %
@Thickness 12.2 - 15.5 mm
>= 14 %
@Thickness 0.480 - 0.610 in
in 2 in. (50 mm)
Modulus of Elasticity 83.0 GPa12000 ksi
 
Thermal PropertiesMetricEnglishComments
CTE, linear  19.7 µm/m-°C
@Temperature 20.0 - 100 °C
10.9 µin/in-°F
@Temperature 68.0 - 212 °F
Estimated from pure Ag
 20.0 µm/m-°C
@Temperature 20.0 - 250 °C
11.1 µin/in-°F
@Temperature 68.0 - 482 °F
Estimated from pure Ag
 20.6 µm/m-°C
@Temperature 20.0 - 500 °C
11.4 µin/in-°F
@Temperature 68.0 - 932 °F
Estimated from pure Ag
Specific Heat Capacity 0.230 J/g-°C0.0550 BTU/lb-°FEstimated from pure Ag
 
Component Elements PropertiesMetricEnglishComments
Magnesium, Mg <= 0.25 %<= 0.25 %
Nickel, Ni 0.25 %0.25 %
Silver, Ag 95.5 %95.5 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
50Ag-50Pd Alloy, Annealed
60Ag-40Pd Alloy, Annealed
90Ag-10Pd Alloy, Annealed
97Ag-3Pd Alloy, Annealed
99Ag-1Pd Alloy, Annealed

MPAgM4 / 12519

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.