MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

INEOS Styrolution Luran® 348Q Crystal Clear Transparent 77850 SAN
Categories: Polymer; Thermoplastic; SAN Polymer; Styrene Acrylonitrile (SAN), Transparent

Material Notes: Description: Highly transparent grade with low natural color.

Information provided by STYROLUTION, which is a joint venture between BASF and INEOS

Key Words: 348 Q
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.08 g/cc0.0390 lb/in³ISO 1183
Moisture Absorption at Equilibrium 0.20 %0.20 %23°C/50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0030 - 0.0070 cm/cm0.0030 - 0.0070 in/in
Melt Flow  20.52 g/10 min
@Load 10.0 kg,
Temperature 220 °C
20.52 g/10 min
@Load 22.0 lb,
Temperature 428 °F
ISO 1133
 29.16 g/10 min
@Load 21.6 kg,
Temperature 200 °C
29.16 g/10 min
@Load 47.6 lb,
Temperature 392 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 7777ISO 2039-2
Ball Indentation Hardness 160 MPa
@Load 36.5 kg,
Time 30.0 sec
23200 psi
@Load 80.5 lb,
Time 0.00833 hour
ISO 2039-1
Tensile Strength at Break 70.0 MPa10200 psiISO 527-1/-2
Elongation at Break 2.5 %2.5 %ISO 527-1/-2
Tensile Modulus 3.60 GPa522 ksiISO 527-1/-2
Flexural Strength 115 MPa16700 psiISO 178
Izod Impact, Notched (ISO) 1.50 kJ/m²0.714 ft-lb/in²ISO 180/A
Charpy Impact Unnotched 1.40 J/cm²
@Temperature 23.0 °C
6.66 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched 0.150 J/cm²
@Temperature 23.0 °C
0.714 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+14 ohm-cm1.00e+14 ohm-cmIEC 60093
Surface Resistance >= 1.00e+15 ohm>= 1.00e+15 ohmIEC 60093
Dielectric Constant  2.8
@Frequency 1e+6 Hz
2.8
@Frequency 1e+6 Hz
IEC 60250
 2.9
@Frequency 100 Hz
2.9
@Frequency 100 Hz
IEC 60250
Dielectric Strength 37.0 kV/mm940 kV/inK20/P50; IEC 60243-1
Dissipation Factor  0.0040
@Frequency 100 Hz
0.0040
@Frequency 100 Hz
IEC 60250
 0.0070
@Frequency 1e+6 Hz
0.0070
@Frequency 1e+6 Hz
IEC 60250
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 70.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
38.9 µin/in-°F
@Temperature 73.4 - 176 °F
ISO 11359-1/-2
Thermal Conductivity 0.170 W/m-K1.18 BTU-in/hr-ft²-°FDIN 52612-1
Maximum Service Temperature, Air 85.0 °C185 °F
Deflection Temperature at 0.46 MPa (66 psi) 99.0 °C210 °FISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 86.0 °C187 °FISO 75-1/-2
Vicat Softening Point 105 °C221 °FVST B50; ISO 306
Flammability, UL94 HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
IEC 60695-11-10
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 90 %90 %transparent; thickness not quantified
 
Processing PropertiesMetricEnglishComments
Melt Temperature 200 - 250 °C392 - 482 °FInjection Molding
Mold Temperature 40.0 - 80.0 °C104 - 176 °FInjection Molding
Drying Temperature 80.0 °C176 °FPre-drying
Dry Time 2 - 4 hour2 - 4 hourPre-drying
 
Descriptive Properties
ColorTransparent 77850
Commercial StatusEurope
Primary Processing TechniqueInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
INEOS Styrolution Luran® 378P Crystal Clear Transparent SAN
INEOS Styrolution Luran® 368R Crystal Clear Transparent 77851 SAN
INEOS Styrolution Luran® 358N SAN
INEOS Styrolution Luran® HH-120 Alpha-Methylstyrene Acrylonitrile
Chi Mei Kibisan® PN-106 L150 SAN

PBASG0596 / 132229

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.