MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Techmer ES Elastoblend® TPX-PA6/6 97058 BK 32% Mineral Filled
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 30% Mineral Filled; Nylon 66, Mineral Filled, Impact Grade

Material Notes: Availability: North America

Forms: Pellets

Filler/Reinforcement: Mineral Fiber Reinforcement, 33% Filler by Weight

Additive: Impact Modifier and Lubricant

Features: Impact Modified and Lubricated

UL File Number: E157318

Appearance: Black

Processing Method: Injection Molding

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.42 g/cc0.0513 lb/in³ASTM D792
Water Absorption 0.70 %
@Time 86400 sec
0.70 %
@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.010 cm/cm
@Thickness 3.17 mm
0.010 in/in
@Thickness 0.125 in
ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 120120ASTM D785
Tensile Strength 77.2 MPa11200 psiASTM D638
Elongation at Yield 16 %16 %ASTM D638
Flexural Yield Strength 116 MPa16800 psiASTM D790
Flexural Modulus 4.52 GPa655 ksiASTM D790
Izod Impact, Notched 1.01 J/cm
@Thickness 3.17 mm
1.90 ft-lb/in
@Thickness 0.125 in
ASTM D256
Izod Impact, Unnotched 14.9 J/cm
@Thickness 3.17 mm
28.0 ft-lb/in
@Thickness 0.125 in
ASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 2.00e+13 ohm-cm2.00e+13 ohm-cmASTM D257
Dielectric Strength 15.0 kV/mm380 kV/inMethod A (Short-Time); ASTM D149
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 54.0 µm/m-°C30.0 µin/in-°FASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 216 °C420 °FUnannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 73.9 °C165 °FUnannealed; ASTM D648
Flammability, UL94 HBHB

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
FKuR Kunststoff Fibrolon® P 7550 Wood-Plastic Compound, Fiber Reinforced
Techmer ES HiFill® TPX-PBT-98010 BN069
Techmer ES Plastiblend® PA6 GF20 RM BK Nylon 6
Techmer ES HiFill® PA6 IM 0240 Impact Modified
FKuR Kunststoff Fibrolon® F 8530 Biodegradable Wood-Plastic Compound, Fiber Reinforced

PTPC1131 / 137069

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.