MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

DuPont Mobility and Materials Delrin® 930MF ® NC000 Mineral Filled Acetal  (discontinued **)
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Copolymer, Mineral Filled

Material Notes: Delrin® 930MF is a new 30% mineral filled acetal with high modulus. It has good flow, low warpage, and a wide processing window.

Information provided by DuPont

Information provided by DuPont; The Delrin product line was sold by DuPont in 2023 but this specific grade was discontinued prior to the sale

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.60 g/cc0.0578 lb/in³ISO 1183
Water Absorption 0.20 %0.20 %24h immersion; ISO 62
Linear Mold Shrinkage, Flow 0.014 cm/cm0.014 in/inISO 294-4
Linear Mold Shrinkage, Transverse 0.013 cm/cm0.013 in/inISO 294-4
Melt Flow 20 g/10 min20 g/10 min190°C, 2.16 kg; ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 44.5 MPa6450 psiISO 527-1/-2
Elongation at Break 20 %20 %Nominal; ISO 527-1/-2
Elongation at Yield 4.0 %4.0 %ISO 527-1/-2
Tensile Modulus 4.20 GPa609 ksiISO 527-1/-2
Flexural Modulus 4.10 GPa595 ksiISO 178
Izod Impact, Notched (ISO) 4.80 kJ/m²2.28 ft-lb/in²ISO 180/1A
Charpy Impact Unnotched 8.00 J/cm²38.1 ft-lb/in²ISO 179/1eU
Charpy Impact, Notched 0.460 J/cm²2.19 ft-lb/in²ISO 179/1eA
 0.400 J/cm²
@Temperature -30.0 °C
1.90 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
CTE, linear 94.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
52.2 µin/in-°F
@Temperature 73.4 - 131 °F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 104 µm/m-°C
@Temperature 23.0 - 55.0 °C
57.8 µin/in-°F
@Temperature 73.4 - 131 °F
ISO 11359-1/-2
Melting Point 168 °C334 °F10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 154 °C309 °FISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 101 °C214 °FISO 75-1/-2
 
Processing PropertiesMetricEnglishComments
Melt Temperature 190 - 210 °C374 - 410 °F
Mold Temperature 80.0 - 100 °C176 - 212 °F
Moisture Content <= 0.20 %<= 0.20 %
Hold Pressure 80.0 - 100 MPa11600 - 14500 psi

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDTAL022 / 32342

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.