MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

ASI® MP 52046 & MP 5209 Activator Methacrylate Adhesive
Categories: Polymer; Adhesive; Thermoset; Methacrylate; Methacrylate Adhesive

Material Notes: MP 52046 is a two component no mix acrylic, curing by contact, does not require mixing. Fixture time is under 30 seconds on most substrates. This material has been engineered to bond a wide range of various metal substrates. The material forms a tough durable bond, able to withstand harsh environments, with excellent aging and weathering properties.

Information provided by Adhesive Systems, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.00 g/cc0.0361 lb/in³Uncured. MP 5209
 1.10 g/cc0.0397 lb/in³Uncured. MP 52046
Viscosity  5.0 - 10 cP
@Temperature 25.0 °C
5.0 - 10 cP
@Temperature 77.0 °F
MP 5209
 15000 - 25000 cP
@Temperature 25.0 °C
15000 - 25000 cP
@Temperature 77.0 °F
MP 52046
Storage Temperature 0.000 - 30.0 °C32.0 - 86.0 °FMP 52046
 
Thermal PropertiesMetricEnglishComments
Flash Point >= 87.0 °C>= 189 °FMP 5209
 >= 103 °C>= 217 °FMP 52046
 
Processing PropertiesMetricEnglishComments
Shelf Life  12.0 Month
@Temperature 20.0 °C
12.0 Month
@Temperature 68.0 °F
MP 52046
 12.0 Month
@Temperature 20.0 °C
12.0 Month
@Temperature 68.0 °F
MP 5209
 
Descriptive Properties
Chemical ClassMethacrylate Ester. MP 5209
 Urethane Methacrylate. MP 52046
Color / appearanceAmber liquid. MP 5209
 Amber/Thixotropic. MP 52046

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PASINC9223 / 233589

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.