MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

CeramTec CD 101 Silicon Carbide, SiC-ZrB2
Categories: Ceramic; Carbide

Material Notes: CD101 is a zirconia reinforced silicon carbide designed for maximum hardness.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 3.26 g/cc0.118 lb/in³DIN EN 623-2
Water Absorption 0.00 %0.00 %DIN EN 623-2
Porosity 2.0 %2.0 %closed (approximate vol. %)
Permeability 0.000.00%, Gas
Weibull Modulus 8.08.0DINV ENV 843-5
 
Mechanical PropertiesMetricEnglishComments
Vickers Microhardness 27502750HV 0.5; DINV ENV 843-4
Tensile Strength at Break 330 MPa47900 psiACMA Test #4 / DIN EN 843-1
Tensile Modulus 415 GPa60200 ksiYoung's; DINV ENV 843-2
Flexural Strength 330 MPa47900 psiDIN EN 843-1
 360 MPa52200 psiBending Strength; 4-Point Method (40x4x3 mm³); ASTM-F417
Compressive Strength 2000 MPa290000 psiDIN 51067T1
Poissons Ratio 0.160.16DINV ENV 843-2
Fracture Toughness 3.80 MPa-m½3.46 ksi-in½KIC; DIN 51109
Shear Modulus 179 GPa26000 ksiCalculated
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity  >= 0.10 ohm-cm
@Temperature 500 °C
>= 0.10 ohm-cm
@Temperature 932 °F
 >= 100 ohm-cm
@Temperature 400 °C
>= 100 ohm-cm
@Temperature 752 °F
IEC 672-1
 >= 30000 ohm-cm
@Temperature 20.0 °C
>= 30000 ohm-cm
@Temperature 68.0 °F
IEC 672-1
Dielectric Constant 29
@Frequency 1e+6 Hz
29
@Frequency 1e+6 Hz
IEC 672-1
Dielectric Loss Index 0.20
@Frequency 9.00e+9 Hz
0.20
@Frequency 9.00e+9 Hz
IEC 672-1
 
Thermal PropertiesMetricEnglishComments
CTE, linear  3.50 µm/m-°C
@Temperature 20.0 - 200 °C
1.94 µin/in-°F
@Temperature 68.0 - 392 °F
DIN EN 821-1
 3.50 µm/m-°C
@Temperature 20.0 - 400 °C
1.94 µin/in-°F
@Temperature 68.0 - 752 °F
DIN EN 821-1
 4.50 µm/m-°C
@Temperature 20.0 - 600 °C
2.50 µin/in-°F
@Temperature 68.0 - 1110 °F
DIN EN 821-1
 4.50 µm/m-°C
@Temperature 20.0 - 1000 °C
2.50 µin/in-°F
@Temperature 68.0 - 1830 °F
DIN EN 821-1
Specific Heat Capacity 0.600 J/g-°C
@Temperature 20.0 - 100 °C
0.143 BTU/lb-°F
@Temperature 68.0 - 212 °F
DINV ENV 821-3
Thermal Conductivity 100 W/m-K
@Temperature 20.0 - 100 °C
694 BTU-in/hr-ft²-°F
@Temperature 68.0 - 212 °F
DIN EN 821-2
Maximum Service Temperature, Air 1400 °C2550 °F
Maximum Service Temperature, Inert 1800 °C3270 °F
 
Descriptive Properties
ColorBlack
Thermal Shock Resistance R1 (K)191R1 = [σs (1-µ)] / (α·E)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Silicon Carbide, Alpha SiC
CeramTec Rocar® SiG Silicon Carbide, SiSiC
Silicon Carbide, CVD
Corundum, Aluminum Oxide, Alumina, 99.9%, Al2O3
Silicon Carbide, sublimed

CCERA921 / 107521

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.