MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Aurora Kunststoffe AUROmid® PA 6 HI10 black 9005 PA6, Heat Stabilized, Impact Modified, Conditioned
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Heat Stabilized; Nylon 6, Impact Grade

Material Notes: Product description: AUROmid® PA6 HI10 black Compound is an unfilled, heat stabilized and high impact modified injection molding grade

Typical applications: fasteners, cable channels, housings

Information provided by Aurora Kunststoffe GmbH

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.10 g/cc0.0397 lb/in³ISO 1183
Moisture Absorption at Equilibrium 2.5 %2.5 %50% r.h.; ISO 62
Water Absorption at Saturation 9.0 %9.0 %Water; ISO 62
Linear Mold Shrinkage, Flow 0.013 cm/cm
@Temperature 80.0 °C
0.013 in/in
@Temperature 176 °F
60x60x2, MT; ISO 294-4
Linear Mold Shrinkage, Transverse 0.013 cm/cm
@Temperature 80.0 °C
0.013 in/in
@Temperature 176 °F
60x60x2, MT; ISO 294-4
Storage Temperature <= 30.0 °C<= 86.0 °F
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 55.0 MPa7980 psi50mm/min; ISO 527-1,-2
Elongation at Break >= 100 %>= 100 %50mm/min; ISO 527-1,-2
Tensile Modulus 0.600 GPa87.0 ksi1mm/min; ISO 527-1,-2
Charpy Impact Unnotched NBNBISO 179-1eU

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PAUROK101 / 249795

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.