MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BASF Ultradur® B 4040 G6 HR BK15029 PBT/PET, 30% Glass Fiber Reinforced
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); PBT + PET Blend, Glass Filled

Material Notes: Product Description: Ultradur® B 4040 G6 HR BK15029 is a hydrolysis resistant, 30% glass reinforced PBT/PET blend, exhibiting good mechanical properties and melt flow properties. Applications: Ultradur B 4040 G6 HR BK15029 is developed for solar and E/E applications.

Availability: North America

Filler/Reinforcement: Glass Fiber, 30% Filler by Weight

Features: Good Flow; Hydrolysis Resistant

Use: Electrical/Electronic Applications; Solar Panels

Agency Ratings: EC 1907/2006 (REACH)

RoSH Compliance: RoSH Compliant

Appearance: Black

Form: Pellets

Processing Method: Injection Molding

Information provided by BASF Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.55 g/cc0.0560 lb/in³ISO 1183
Viscosity Number 97 cm³/g0.97 dl/gReduced Viscosity; ISO 1628
Maximum Moisture Content 0.0200.020
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 127 MPa18400 psiISO 527-2
Elongation at Break 2.7 %2.7 %ISO 527-2
Tensile Modulus 8.89 GPa1290 ksiISO 527-1
Flexural Strength 220 MPa31900 psiISO 178
Flexural Modulus 9.03 GPa1310 ksiISO 178
Izod Impact, Notched (ISO)  7.14 kJ/m²
@Temperature -40.0 °C
3.40 ft-lb/in²
@Temperature -40.0 °F
ISO 180
 8.19 kJ/m²
@Temperature 22.8 °C
3.90 ft-lb/in²
@Temperature 73.0 °F
ISO 180
Charpy Impact Unnotched 5.88 J/cm²28.0 ft-lb/in²ISO 179
Charpy Impact, Notched  0.777 J/cm²
@Temperature -30.0 °C
3.70 ft-lb/in²
@Temperature -22.0 °F
ISO 179
 0.861 J/cm²
@Temperature 22.8 °C
4.10 ft-lb/in²
@Temperature 73.0 °F
ISO 179
 
Thermal PropertiesMetricEnglishComments
Melting Point 223 °C433 °FISO 3146
Deflection Temperature at 1.8 MPa (264 psi) 200 °C392 °FUnannealed; ISO 75-2/A
 
Processing PropertiesMetricEnglishComments
Melt Temperature 250 - 275 °C482 - 527 °F
Mold Temperature 40.0 - 70.0 °C104 - 158 °F
Drying Temperature 100 - 120 °C212 - 248 °F
Dry Time 4.00 hour4.00 hour
Injection Pressure 3.50 - 12.5 MPa508 - 1810 psi
Back Pressure <= 1.00 MPa<= 145 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PBASG2146 / 310839

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.