HiDura™ D2X NT is a medium-high viscosity PA612 grade. It is suitable for monofilament, film, and profile extrusion applications. It exhibits low moisture absorption, good chemical resistance, dimensional stability, and high impact resilience. PA612 offers a unique balance of thermal, mechanical, and physical properties.Information provided by Ascend Performance Materials. |