MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Cosmic Plastics 6130 Long Glass Fiber Filled Ortho Diallyl Phthalate Molding Compound  (discontinued **)
Categories: Polymer; Thermoset; Diallyl Phthalate (DAP); Diallyl Phthalate (DAP) Molding Compound, Long Glass Fiber Filled; Filled/Reinforced Thermoset

Material Notes:

Data provided by the manufacturer.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.82 g/cc0.0658 lb/in³
Apparent Bulk Density 0.300 g/cc0.0108 lb/in³
Water Absorption 0.27 %0.27 %48 hrs, 50°C
Linear Mold Shrinkage 0.0010 - 0.0040 cm/cm0.0010 - 0.0040 in/intypical.
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 41.0 - 55.0 MPa5950 - 7980 psi
Flexural Strength 103 MPa14900 psi
Compressive Strength 186 MPa27000 psi
Izod Impact, Notched 2.40 J/cm4.50 ft-lb/in
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity >= 1.00e+17 ohm-cm>= 1.00e+17 ohm-cm
Surface Resistance >= 1.00e+17 ohm>= 1.00e+17 ohm
Dielectric Constant  4.1
@Frequency 1000 Hz
4.1
@Frequency 1000 Hz
Wet
 4.3
@Frequency 1e+6 Hz
4.3
@Frequency 1e+6 Hz
Wet
Dielectric Strength 14.0 kV/mm356 kV/inWet, Step by Step
Dissipation Factor  0.0090
@Frequency 1000 Hz
0.0090
@Frequency 1000 Hz
Wet
 0.012
@Frequency 1e+6 Hz
0.012
@Frequency 1e+6 Hz
Wet
Arc Resistance 160 sec160 sec
 
Thermal PropertiesMetricEnglishComments
CTE, linear 24.0 µm/m-°C
@Temperature 20.0 °C
13.3 µin/in-°F
@Temperature 68.0 °F
Deflection Temperature at 1.8 MPa (264 psi) 260 °C500 °FHeat Distortion temperature
 
Processing PropertiesMetricEnglishComments
Processing Temperature 135 - 165 °C275 - 329 °FMolding temperature

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese Zenite® 6130 WT010 30% GF LCP (Extended Tabular Temperature Data)
Celanese Zenite® 6130 BK010 LCP, 30% glass reinforced (Extended Tabular Temperature Data)
Universal Wire Works 6130 (AMS 6462) Low Alloy Steel Welding Wire
DuPont Mobility and Materials Crastin® 6130 NC010 PBT
Cosmic Plastics D69/6130 Long Glass Fiber Filled Diallyl Iso-Phthalate Molding Compound

PAESCD / 22936

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.