MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Dow UCON™ LB-1145 Fluids and Lubricants
Categories: Fluid; Lubricant

Material Notes: A moderate-viscosity fluid that provides emolliency, solvency, and slip in skin lotions, antiperspirants, eye makeup removers, and deodorants. At the same time, it can offer a number of other benefits, such as the ability to efficiently wet pigments. A water insoluble PAG. INCI Name: PPG-33 Butyl Ether

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density  0.934 g/cc
@Temperature 100 °C
0.0337 lb/in³
@Temperature 212 °F
 0.982 g/cc
@Temperature 40.0 °C
0.0355 lb/in³
@Temperature 104 °F
 1.00 g/cc
@Temperature 20.0 °C
0.0361 lb/in³
@Temperature 68.0 °F
Viscosity Measurement 214214Index; ASTM D2270, IP 226
 220220ISO Viscosity Grade
 5600056000@ -18°C, [SUS], Saybolt
Saybolt Viscosity at 100°F 1145 SUS1145 SUS
Viscosity Measure 2470 cSt
@Temperature 0.000 °C
2470 cSt
@Temperature 32.0 °F
Saybolt Viscosity at 210°F 177 SUS177 SUS
Kinematic Viscosity at 40°C (104°F) 230 cSt230 cSt
Kinematic Viscosity at 100°C (212°F) 36.9 cSt36.9 cSt
Molecular Weight 2080 g/mol2080 g/mol
 
Thermal PropertiesMetricEnglishComments
CTE, linear 0.000800 µm/m-°C
@Temperature 55.0 °C
0.000444 µin/in-°F
@Temperature 131 °F
Pour Point -29.0 °C-20.2 °FASTM D97, IP 15
Flash Point 191 °C376 °FPMCC; ASTM D93, IP 34
 235 °C455 °FCOC; ASTM D93, IP 36
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.44991.4499
 
Descriptive Properties
Weight per Gallon8.34 lb

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDOW2008 / 183655

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.