MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Isoflon MFA TFE/Perfluoromethylvinylether Copolymer
Categories: Polymer; Thermoplastic; Fluoropolymer; TFE/Perfluoromethylvinylether Copolymer (MFA)

Material Notes: Fluoropolymer material specifications.

Information provided by Isoflon.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.12 - 2.17 g/cc2.12 - 2.17 g/ccISO 12086
Water Absorption 0.025 %0.025 %DIN 53 495
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 57 - 6057 - 60DIN 53 505
Tensile Strength 28.0 - 36.0 MPa4060 - 5220 psiDIN 53455
Elongation at Break 250 - 360 %250 - 360 %DIN 53455
Tensile Modulus 0.440 - 0.480 GPa63.8 - 69.6 ksiDIN 53457
Coefficient of Friction, Dynamic 0.280.28on steel
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 30.0 - 35.0 kV/mm762 - 889 kV/inDIN 53481
 
Thermal PropertiesMetricEnglishComments
CTE, linear 120 µm/m-°C
@Temperature 20.0 - 100 °C
66.7 µin/in-°F
@Temperature 68.0 - 212 °F
Thermal Conductivity 0.200 W/m-K1.39 BTU-in/hr-ft²-°FDIN 52612
Maximum Service Temperature, Air 230 °C446 °FContinuous
Minimum Service Temperature, Air -150 °C-238 °FContinuous

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PISOFL961 / 123349

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.