AT 234R homopolymer is recommended for higher pressure series pipe applications such as municipal water service pipe. It complies with Code of Federal Regulation 21 CFR Section 177.1520 subject to extraction limitations for specific end use applications. Additives: Applications: Tubes & Pipes Information provided by Celanese Corporation. |
higher pressure series pipe applications such as municipal water service pipe |