MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Mid-Mountain Materials SILTEX® XS-150 Silica Yarn
Categories: Ceramic; Glass; Glass Fiber; Oxide; Silicon Oxide

Material Notes: SILTEX® SILICA YARN XS-150 is comprised of continuous filament, amorphous silica fibers and offers superior protection in electrical applications, as well as excellent resistance to thermal shock and high dielectric strength. SILTEX® SILICA YARN XS-150 is highly porous, and will operate continuously at temperatures up to 1800°F (982°C). Lubricated with PTFE for ease of handling and improved abrasion resistance, SILTEX® SILICA YARN XS-150 has minimal shrinkage at service temperatures.

Information provided by Mid-Mountain Materials

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Filament Diameter 508 µm508 µm
Fiber Count 15.0 dtex13.5 denier
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 982 °C1800 °FContinuous
Shrinkage 7.0 %
@Temperature 982 °C
7.0 %
@Temperature 1800 °F
 
Component Elements PropertiesMetricEnglishComments
SiO2 98 %98 %
 
Descriptive Properties
CoatingPTFE
Coating (%)7PTFE
Spool Weight (lbs)0.25
Tensile Strength (lbs)3.8
Yield (ly/lb)3300

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ceradyne Thermo-Sil® Isomolded™ Fused Silica
96% Silica Consolidated Reconstructed Glass
DuPont™ Kevlar® 49 Aramid Fiber
DuPont™ Kevlar® 149 Aramid Fiber, diam. 12 µm
Saint-Gobain Chemfab® 1580 PTFE Coated Fiberglass Conveyor Belting

CMID07a / 141225

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.