MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LyondellBasell Petrothene® NA317009 Low Density Polyethylene, Film Extrusion Grade  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Blow Molding Grade

Material Notes: PETROTHENE NA317 is a series of homopolymer resins designed for household wrap and other applications requiring high clarity and good impact strength.

Regulatory Status: The base resin NA317 meets the requirements of the Food and Drug Administration, regulation 21CFR 177.1520. This regulation allows the use of this olefin polymer in "...articles or components of articles intended for use in contact with food." Specific limitations or conditions of use may apply.

Specific recommendations for processing NA317 can only be made when the processing conditions, equipment and end use are known.

This product is from the former Equistar product line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.925 g/cc0.0334 lb/in³ASTM D1505
Thickness 31.8 microns1.25 mil
Melt Flow 2.0 g/10 min2.0 g/10 minASTM D1238
Antiblock Level 0.000 ppm0.000 ppm
Slip Level 0.000 ppm0.000 ppm
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, TD 11.0 MPa1600 psiASTM D882
Film Elongation at Break, MD 300 %300 %ASTM D882
Film Elongation at Break, TD 450 %450 %ASTM D882
Elmendorf Tear Strength MD 360 g360 gASTM D1922
Elmendorf Tear Strength TD 400 g400 gASTM D1922
Dart Drop 2.20 g/micron56.0 g/milF50; ASTM D1709
Film Tensile Strength at Break, MD 27.6 MPa4000 psiASTM D882
Film Tensile Strength at Break, TD 20.7 MPa3000 psiASTM D882
1% Secant Modulus, MD 207 MPa30000 psiASTM D882
1% Secant Modulus, TD 248 MPa36000 psiASTM D882
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 100 °C212 °FASTM D1525
 
Optical PropertiesMetricEnglishComments
Haze 4.0 %4.0 %ASTM D1003
Gloss 80 %80 %45°; ASTM D2457
 
Processing PropertiesMetricEnglishComments
Melt Temperature 191 °C375 °F
Die Opening 0.0635 cm0.0250 in
Blow-up Ratio (BUR) 2.02.0
 
Compliance PropertiesMetricEnglishComments
FDA YesYes

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEQU0831 / 104187

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.